Physico-chemical and electrical properties of bismuth chromate solid solutions

Bismuth chromium solid solutions, with a general formula Bi6-xCr2Oδ, where -1 ≤ x ≤ 2, were successfully synthesized via the conventional solid state method. The phases of the synthesized samples were determined by X-ray diffraction (XRD) analysis. The properties of single-phase compounds were chara...

Full description

Bibliographic Details
Main Authors: Wong, Y. C., Tan, Yen Ping
Format: Article
Language:English
Published: Universiti Putra Malaysia Press 2013
Online Access:http://psasir.upm.edu.my/id/eprint/40491/
http://psasir.upm.edu.my/id/eprint/40491/1/29.%20Physico-Chemical%20and%20Electrical%20Properties%20of%20Bismuth%20Chromate.pdf
_version_ 1848849441712242688
author Wong, Y. C.
Tan, Yen Ping
author_facet Wong, Y. C.
Tan, Yen Ping
author_sort Wong, Y. C.
building UPM Institutional Repository
collection Online Access
description Bismuth chromium solid solutions, with a general formula Bi6-xCr2Oδ, where -1 ≤ x ≤ 2, were successfully synthesized via the conventional solid state method. The phases of the synthesized samples were determined by X-ray diffraction (XRD) analysis. The properties of single-phase compounds were characterized by using differential thermal analysis (DTA), thermal gravimetric analysis (TGA), AC impedance spectroscopy, and inductively coupled plasma-atomic emission spectroscopy (ICP-AES). The occurrence of phase transitions was confirmed by DTA and TGA, where a thermal event was observed by DTA at around 800°C. In addition, TGA studies also showed that there was a weight loss at around 800°C. Elemental analysis of Bi6Cr2O15and its solid solutions by ICP-AES showed a good agreement between the expected value and the experimental value on the compositions, with no evidence of any systematic deviation from stoichiometric. Electrical properties of Bi6Cr2O15and its solid solutions were investigated by using AC impedance spectroscopy from 300°C to 650°C. Ionic conductivity increased with the increasing temperature and bismuth content, and the best ionic conductivity was observed for Bi7Cr2O16.5. The activation energy (Ea) of Bi6Cr2O15and its solid solutions were in the range of 1.22-1.32 eV.
first_indexed 2025-11-15T09:50:27Z
format Article
id upm-40491
institution Universiti Putra Malaysia
institution_category Local University
language English
last_indexed 2025-11-15T09:50:27Z
publishDate 2013
publisher Universiti Putra Malaysia Press
recordtype eprints
repository_type Digital Repository
spelling upm-404912015-11-04T06:48:43Z http://psasir.upm.edu.my/id/eprint/40491/ Physico-chemical and electrical properties of bismuth chromate solid solutions Wong, Y. C. Tan, Yen Ping Bismuth chromium solid solutions, with a general formula Bi6-xCr2Oδ, where -1 ≤ x ≤ 2, were successfully synthesized via the conventional solid state method. The phases of the synthesized samples were determined by X-ray diffraction (XRD) analysis. The properties of single-phase compounds were characterized by using differential thermal analysis (DTA), thermal gravimetric analysis (TGA), AC impedance spectroscopy, and inductively coupled plasma-atomic emission spectroscopy (ICP-AES). The occurrence of phase transitions was confirmed by DTA and TGA, where a thermal event was observed by DTA at around 800°C. In addition, TGA studies also showed that there was a weight loss at around 800°C. Elemental analysis of Bi6Cr2O15and its solid solutions by ICP-AES showed a good agreement between the expected value and the experimental value on the compositions, with no evidence of any systematic deviation from stoichiometric. Electrical properties of Bi6Cr2O15and its solid solutions were investigated by using AC impedance spectroscopy from 300°C to 650°C. Ionic conductivity increased with the increasing temperature and bismuth content, and the best ionic conductivity was observed for Bi7Cr2O16.5. The activation energy (Ea) of Bi6Cr2O15and its solid solutions were in the range of 1.22-1.32 eV. Universiti Putra Malaysia Press 2013 Article PeerReviewed application/pdf en http://psasir.upm.edu.my/id/eprint/40491/1/29.%20Physico-Chemical%20and%20Electrical%20Properties%20of%20Bismuth%20Chromate.pdf Wong, Y. C. and Tan, Yen Ping (2013) Physico-chemical and electrical properties of bismuth chromate solid solutions. Pertanika Journal of Science & Technology, 21 (1). pp. 97-110. ISSN 0128-7680; ESSN: 2231-8526 http://www.pertanika.upm.edu.my/Pertanika%20PAPERS/JST%20Vol.%2021%20%281%29%20Jan.%202013/08.%20%20Page%2097-110.pdf
spellingShingle Wong, Y. C.
Tan, Yen Ping
Physico-chemical and electrical properties of bismuth chromate solid solutions
title Physico-chemical and electrical properties of bismuth chromate solid solutions
title_full Physico-chemical and electrical properties of bismuth chromate solid solutions
title_fullStr Physico-chemical and electrical properties of bismuth chromate solid solutions
title_full_unstemmed Physico-chemical and electrical properties of bismuth chromate solid solutions
title_short Physico-chemical and electrical properties of bismuth chromate solid solutions
title_sort physico-chemical and electrical properties of bismuth chromate solid solutions
url http://psasir.upm.edu.my/id/eprint/40491/
http://psasir.upm.edu.my/id/eprint/40491/
http://psasir.upm.edu.my/id/eprint/40491/1/29.%20Physico-Chemical%20and%20Electrical%20Properties%20of%20Bismuth%20Chromate.pdf