Carbonitridation of mechanically activated mixtures of zircon and carbon

Two different stoichiometries of zircon (ZrSiO4) and activated carbon (C:zircon molar ratios of 3:1 and 6:1) were milled together at for 5 h and subjected to thermo-gravimetric analysis (TGA). TGA runs were performed under argon and nitrogen atmospheres. The main mass loss reaction started at around...

Full description

Bibliographic Details
Main Authors: Setoudeh, N., Welham, Nick
Format: Journal Article
Published: Elsevier B.V. 2014
Online Access:http://hdl.handle.net/20.500.11937/44067