Sidewall design to improve lining life in a platinum smelting furnace

The matte/slag tidal zone in a platinum smelting furnace is subject to severe process conditions which can often lead to premature failure of the lining. The MgO-FeO-Si02 slag is aggressive to refractory bricks, whilst the Ni-Cu-Fe-S matte is aggressive to water-cooled copper cooling elements, and c...