Compression strength and microhardness of recycling milled aluminium (AA6061) for various binder
In this investigation, AA6061 milled particle size was fabricated by milling machine plus compacted by hydraulic press in room temperature. Finally, sintering in the temperature range of 552 OC. The samples were compacted by 9 tons. The holding time was 20 mins. Three groups of specimens were chosen...
Main Authors: | Mahdi, Ahmed Sahib, Mustapa, Mohammad Sukri, Lajis, Mohd Amri, Abd Rashid, Mohd Warikh |
---|---|
Format: | Article |
Published: |
Research Publish Journals
2016
|
Subjects: | |
Online Access: | http://eprints.uthm.edu.my/8955/ |
Similar Items
-
Effect of sintering temperature on compression strength and microhardness of recycling aluminium alloy AA6061 through ball mill process
by: Mahdi, Ahmed Sahib, et al.
Published: (2016) -
Effect of compaction pressure on physical properties of milled aluminium chip (AA6061)
by: Mahdi, Ahmed Sahib, et al.
Published: (2015) -
Physical properties of recycling milled aluminium chip (AA6061) for various sintering temperature
by: Mustapa, Mohd Sukri, et al.
Published: (2016) -
Effect of holding time on mechanical properties of recycling aluminium alloy AA6061 through ball mill process
by: Mahdi, Ahmed Sahib, et al.
Published: (2015) -
The effect of cold compacting parameters for producing recycles aluminium by milling process
by: Mahdi, Ahmed Sahib, et al.
Published: (2016)