Oxidation of pure aluminium granules during in-situ melting

Oxidation behaviour of in-situ melted pure aluminium was investigated. The granules were heated in ceramic investment casting moulds between 700 and 850oC, for the duration of 30 and 60 min in atmospheric air using high temperature muffle furnace. The product was visually inspected macroscopically f...