Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes

The longitudinal and shear sound velocities in colossal magnetoresistive material La0.67Ca0.33MnO3 sintered at 1100, 1250 and 1350 °C with average grain size 1, 3 and 5 μm, respectively, have been measured from 80 to 300 K using the pulse-echo-overlap method. A pronounced increase in the longitudina...

Full description

Bibliographic Details
Main Authors: Ewe, L.S., Hamadneh, I., Salama, H.A., Abd-Shukor, R.
Published: 2018
Online Access:http://dspace.uniten.edu.my/jspui/handle/123456789/9422
id uniten-123456789-9422
recordtype eprints
spelling uniten-123456789-94222018-02-28T23:58:33Z Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes Ewe, L.S. Hamadneh, I. Salama, H.A. Abd-Shukor, R. The longitudinal and shear sound velocities in colossal magnetoresistive material La0.67Ca0.33MnO3 sintered at 1100, 1250 and 1350 °C with average grain size 1, 3 and 5 μm, respectively, have been measured from 80 to 300 K using the pulse-echo-overlap method. A pronounced increase in the longitudinal sound velocity was observed in all samples around the insulator-metal transition temperature (TIM∼272 K). XRD patterns showed the orthorhombic structure for all samples. The longitudinal and shear velocities showed the largest hysteresis for the sample with 3 μm grain size. A step-like shear sound velocity anomaly near 120 K during cooling or warming was observed to be dependent on the grain size. © 2007 Elsevier B.V. All rights reserved. 2018-02-28T23:58:33Z 2018-02-28T23:58:33Z 2008 http://dspace.uniten.edu.my/jspui/handle/123456789/9422
repository_type Digital Repository
institution_category Local University
institution Universiti Tenaga Nasional
building UNITEN Institutional Repository
collection Online Access
description The longitudinal and shear sound velocities in colossal magnetoresistive material La0.67Ca0.33MnO3 sintered at 1100, 1250 and 1350 °C with average grain size 1, 3 and 5 μm, respectively, have been measured from 80 to 300 K using the pulse-echo-overlap method. A pronounced increase in the longitudinal sound velocity was observed in all samples around the insulator-metal transition temperature (TIM∼272 K). XRD patterns showed the orthorhombic structure for all samples. The longitudinal and shear velocities showed the largest hysteresis for the sample with 3 μm grain size. A step-like shear sound velocity anomaly near 120 K during cooling or warming was observed to be dependent on the grain size. © 2007 Elsevier B.V. All rights reserved.
author Ewe, L.S.
Hamadneh, I.
Salama, H.A.
Abd-Shukor, R.
spellingShingle Ewe, L.S.
Hamadneh, I.
Salama, H.A.
Abd-Shukor, R.
Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes
author_facet Ewe, L.S.
Hamadneh, I.
Salama, H.A.
Abd-Shukor, R.
author_sort Ewe, L.S.
title Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes
title_short Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes
title_full Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes
title_fullStr Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes
title_full_unstemmed Sound velocity in perovskite manganites La0.67Ca0.33MnO3 with different grain sizes
title_sort sound velocity in perovskite manganites la0.67ca0.33mno3 with different grain sizes
publishDate 2018
url http://dspace.uniten.edu.my/jspui/handle/123456789/9422
first_indexed 2018-09-05T08:12:38Z
last_indexed 2018-09-05T08:12:38Z
_version_ 1610754459858632704