Obtaining of Ni/NiO nanopowder from aqua solutions of Ni(CH3COO)2 ammonia complexes
Ni/NiO nanopowders have been prepared by using thermal decomposition of aqua solutions of nickel acetate ammine complexes in air at the annealing temperature range of 300°C to 500°C, time of decomposition from 30 to 180 min, and ammonia content in initial complex 3.6 to 9.55 mol/mol Ni2+. Chemical c...