Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system

Metal Injection Moulding (MIM) has undergone development of various binder systems with the aims of shortening the overall debinding time duration. In the present work, binder system based on biopolymer has been utilised in injection moulding of hip stem CoCrMo alloy powder. The feedstock consist...

Full description

Bibliographic Details
Main Authors: Omar, Mohd Afian, Abdullah, Noorsyakirah, Sauti, Rosliza, Mohd Zainon, Nurazilah, Johari, Nurhaslina, Zulkifly, Ahmad Hafiz, Baharuddin, Mohd Yusof
Format: Article
Language:English
Published: Trans Tech Publications Ltd., Switzerland 2016
Subjects:
Online Access:http://irep.iium.edu.my/49242/
http://irep.iium.edu.my/49242/
http://irep.iium.edu.my/49242/
http://irep.iium.edu.my/49242/1/Metal_Injection_Moulding_of_Hip_Stem_CoCrMo_Alloy_Powder_using.pdf
id iium-49242
recordtype eprints
spelling iium-492422017-10-16T09:09:34Z http://irep.iium.edu.my/49242/ Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system Omar, Mohd Afian Abdullah, Noorsyakirah Sauti, Rosliza Mohd Zainon, Nurazilah Johari, Nurhaslina Zulkifly, Ahmad Hafiz Baharuddin, Mohd Yusof RD701 Orthopedics Metal Injection Moulding (MIM) has undergone development of various binder systems with the aims of shortening the overall debinding time duration. In the present work, binder system based on biopolymer has been utilised in injection moulding of hip stem CoCrMo alloy powder. The feedstock consisted of CoCrMo powder with mean diameter particle size of 16 μm and binder which comprised of major fraction of wax and minor fraction of polyethylene. The moulded part was immersed into n-heptane at 60 °C in order to remove the palm stearin, followed by sintering in a controlled vacuum atmosphere. Results showed that solvent extraction debinding technique allowed complete removal of palm stearin from the injection moulded part within 5 hours without swelling or distortion of the debound part. Lower heating rate is needed during thermal pyrolysis in order to retain the shape due to the thickness of the part. Trans Tech Publications Ltd., Switzerland 2016-01 Article PeerReviewed application/pdf en http://irep.iium.edu.my/49242/1/Metal_Injection_Moulding_of_Hip_Stem_CoCrMo_Alloy_Powder_using.pdf Omar, Mohd Afian and Abdullah, Noorsyakirah and Sauti, Rosliza and Mohd Zainon, Nurazilah and Johari, Nurhaslina and Zulkifly, Ahmad Hafiz and Baharuddin, Mohd Yusof (2016) Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system. Advanced Materials Research, 1133. pp. 334-338. ISSN 1662-8985 http://www.scientific.net/AMR.1133.334 10.4028/www.scientific.net/AMR.1133.334
repository_type Digital Repository
institution_category Local University
institution International Islamic University Malaysia
building IIUM Repository
collection Online Access
language English
topic RD701 Orthopedics
spellingShingle RD701 Orthopedics
Omar, Mohd Afian
Abdullah, Noorsyakirah
Sauti, Rosliza
Mohd Zainon, Nurazilah
Johari, Nurhaslina
Zulkifly, Ahmad Hafiz
Baharuddin, Mohd Yusof
Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system
description Metal Injection Moulding (MIM) has undergone development of various binder systems with the aims of shortening the overall debinding time duration. In the present work, binder system based on biopolymer has been utilised in injection moulding of hip stem CoCrMo alloy powder. The feedstock consisted of CoCrMo powder with mean diameter particle size of 16 μm and binder which comprised of major fraction of wax and minor fraction of polyethylene. The moulded part was immersed into n-heptane at 60 °C in order to remove the palm stearin, followed by sintering in a controlled vacuum atmosphere. Results showed that solvent extraction debinding technique allowed complete removal of palm stearin from the injection moulded part within 5 hours without swelling or distortion of the debound part. Lower heating rate is needed during thermal pyrolysis in order to retain the shape due to the thickness of the part.
format Article
author Omar, Mohd Afian
Abdullah, Noorsyakirah
Sauti, Rosliza
Mohd Zainon, Nurazilah
Johari, Nurhaslina
Zulkifly, Ahmad Hafiz
Baharuddin, Mohd Yusof
author_facet Omar, Mohd Afian
Abdullah, Noorsyakirah
Sauti, Rosliza
Mohd Zainon, Nurazilah
Johari, Nurhaslina
Zulkifly, Ahmad Hafiz
Baharuddin, Mohd Yusof
author_sort Omar, Mohd Afian
title Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system
title_short Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system
title_full Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system
title_fullStr Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system
title_full_unstemmed Metal injection moulding of hip stem CoCrMo alloy powder using palm stearin binder system
title_sort metal injection moulding of hip stem cocrmo alloy powder using palm stearin binder system
publisher Trans Tech Publications Ltd., Switzerland
publishDate 2016
url http://irep.iium.edu.my/49242/
http://irep.iium.edu.my/49242/
http://irep.iium.edu.my/49242/
http://irep.iium.edu.my/49242/1/Metal_Injection_Moulding_of_Hip_Stem_CoCrMo_Alloy_Powder_using.pdf
first_indexed 2018-09-07T06:56:06Z
last_indexed 2018-09-07T06:56:06Z
_version_ 1610930839151968256