Internal oxidation of Ni-Cr-Al alloys under various oxygen partial pressures at 1273 K
Alloys for high temperature application always rely on their ability to form protective, dense Cr2O3 and Al2O3 scales. In case of Ni-Cr binary alloy, a minimum composition of Cr is required for the formation of continuous protective scale. However, addition of small amount of third element such a...
Main Authors: | Ani, Mohd Hanafi, Herman, Sukreen Hana, -, Suryanto, Othman, Raihan |
---|---|
Format: | Article |
Language: | English English |
Published: |
Trans Tech Publications, Switzerland
2012
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/27472/ http://irep.iium.edu.my/27472/ http://irep.iium.edu.my/27472/ http://irep.iium.edu.my/27472/1/internal_oxidation_of_ni-cr-al_alloys_under_various_oxygen_partial_pressures_at_1273k.pdf http://irep.iium.edu.my/27472/4/27472_Internal%20Oxidation%20of%20Ni-Cr-Al%20Alloys%20under%20_SCOPUS.pdf |
Similar Items
-
Studies on initial stage of high temperature oxidation of Fe - 9 to 12% Cr alloys in water vapour environment
by: Kaderi, Akbar, et al.
Published: (2012) -
Observation on void formed in oxide scale of Fe-Cr-Ni alloy at 1073K in dry and humid environments
by: Kaderi, Akbar, et al.
Published: (2011) -
Formation of protective Cr2O3 scale at high temperature and the effect of mass transport in the presence of water vapor
by: Ani, Mohd Hanafi, et al.
Published: (2012) -
The corrosion study of Co-Cr-Ni alloy fabricated by powder metallurgy
by: Othman, Raudhah, et al.
Published: (2010) -
Initial stage oxidation of cr in dry and wet environment at 1073 K and the significant differences of FT – IR spectra produced thereof
by: Kaderi, Akbar, et al.
Published: (2012)