Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature

Recent studies have shown that blending of ground granulated blast furnace slag (GGBFS) with low-calcium fly ash can have significant effects on the setting and early strength development of geopolymers cured at room temperature. This paper presents the shrinkage behaviour of geopolymer concrete mix...

Full description

Bibliographic Details
Main Authors: Deb, Partha, Nath, Pradip, Sarker, Prabir
Format: Journal Article
Published: Elsevier BV 2015
Subjects:
Online Access:http://hdl.handle.net/20.500.11937/10729
id curtin-20.500.11937-10729
recordtype eprints
spelling curtin-20.500.11937-107292017-09-13T14:55:05Z Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature Deb, Partha Nath, Pradip Sarker, Prabir fly ash GGBFS shrinkage room temperature curing geopolymer Recent studies have shown that blending of ground granulated blast furnace slag (GGBFS) with low-calcium fly ash can have significant effects on the setting and early strength development of geopolymers cured at room temperature. This paper presents the shrinkage behaviour of geopolymer concrete mixtures in which class F fly ash was replaced with 10% or 20% GGBFS and the sodium silicate to sodium hydroxide (SS/SH) ratio was either 1.5 or 2.5. Shrinkage of 4 geopolymer and 1 ordinary Portland cement (OPC) concrete mixtures cured at room temperature were studied. Comparisons are made between the shrinkage behaviours of geopolymer concretes with different mixture proportions and those of the OPC concrete. It was found that shrinkage decreased with the increase of slag content and decrease of SS/SH ratio in geopolymer concrete cured at room temperature. The shrinkage of geopolymer concrete up to the age of 180 days was found to be comparable to that of OPC concrete of similar compressive strength. Thus, shrinkage of geopolymer concrete could be reduced to values within the limit recommended in the Australian Standards for normal OPC concrete. 2015 Journal Article http://hdl.handle.net/20.500.11937/10729 10.1016/j.proeng.2015.11.066 Elsevier BV fulltext
repository_type Digital Repository
institution_category Local University
institution Curtin University Malaysia
building Curtin Institutional Repository
collection Online Access
topic fly ash
GGBFS
shrinkage
room temperature curing
geopolymer
spellingShingle fly ash
GGBFS
shrinkage
room temperature curing
geopolymer
Deb, Partha
Nath, Pradip
Sarker, Prabir
Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature
description Recent studies have shown that blending of ground granulated blast furnace slag (GGBFS) with low-calcium fly ash can have significant effects on the setting and early strength development of geopolymers cured at room temperature. This paper presents the shrinkage behaviour of geopolymer concrete mixtures in which class F fly ash was replaced with 10% or 20% GGBFS and the sodium silicate to sodium hydroxide (SS/SH) ratio was either 1.5 or 2.5. Shrinkage of 4 geopolymer and 1 ordinary Portland cement (OPC) concrete mixtures cured at room temperature were studied. Comparisons are made between the shrinkage behaviours of geopolymer concretes with different mixture proportions and those of the OPC concrete. It was found that shrinkage decreased with the increase of slag content and decrease of SS/SH ratio in geopolymer concrete cured at room temperature. The shrinkage of geopolymer concrete up to the age of 180 days was found to be comparable to that of OPC concrete of similar compressive strength. Thus, shrinkage of geopolymer concrete could be reduced to values within the limit recommended in the Australian Standards for normal OPC concrete.
format Journal Article
author Deb, Partha
Nath, Pradip
Sarker, Prabir
author_facet Deb, Partha
Nath, Pradip
Sarker, Prabir
author_sort Deb, Partha
title Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature
title_short Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature
title_full Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature
title_fullStr Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature
title_full_unstemmed Drying Shrinkage of slag blended fly ash geopolymer concrete cured at room temperature
title_sort drying shrinkage of slag blended fly ash geopolymer concrete cured at room temperature
publisher Elsevier BV
publishDate 2015
url http://hdl.handle.net/20.500.11937/10729
first_indexed 2018-09-06T18:45:50Z
last_indexed 2018-09-06T18:45:50Z
_version_ 1610884894862344192