On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process

The objective of this research is to investigate the appropriate range of coagulation bath temperature and polymer solution composition for spinning process in the solvent-free coagulation process and the effect of these parameters on carbon fibers precursor. The fabrication of the precursor fiber i...

Full description

Bibliographic Details
Main Authors: Ismail, Ahmad Fauzi, Rahman, M. A., Mustafa, A.
Format: Conference or Workshop Item
Language:English
Published: 2006
Subjects:
Online Access:http://eprints.utm.my/5464/
http://eprints.utm.my/5464/1/A.F.Ismail2006_OnTheFabricationAndCharacteristicsOfPAN.pdf
_version_ 1848891059040419840
author Ismail, Ahmad Fauzi
Rahman, M. A.
Mustafa, A.
author_facet Ismail, Ahmad Fauzi
Rahman, M. A.
Mustafa, A.
author_sort Ismail, Ahmad Fauzi
building UTeM Institutional Repository
collection Online Access
description The objective of this research is to investigate the appropriate range of coagulation bath temperature and polymer solution composition for spinning process in the solvent-free coagulation process and the effect of these parameters on carbon fibers precursor. The fabrication of the precursor fiber in the solvent-free coagulation process was carried out it a low residence time. The precursor fibers with excellent axial orientation and less number of micro-pores possess superior mechanical properties and enhance the performance of resulting carbon fibers. In the first stage of this study, the PAN polymer solution was prepared with incorporation of acrylamide as an additive. Th PAN/AM fibers were produced using a simple dry-wet spinning process. The PAN/AM fibers were then subjected to the oxidation process at 250 C in an oxygen-containing- atmosphere before underwent the carbonization process at 1000 °C. Through these studies, that a semi-dilute solution (18 wt.%) was found to be the most suitable polymer composition for the PAN/AM fibers fabrication at room temperature. It eased the fabrication process and produced the PAN/AM fibers with better mechanical properties. The PAN/AM fibers produced at coagulation bath temperature of 13 °C exhibited the excellent mechanical properties. At the coagulation bath temperature of 13 °C, the inward diffusion of non-solvent was still slow and consequendy reduced the number of micro-pores and fit for the drawing process. The ratio of carbon fiber to precursor modulus (Ec/Ep) was calculated to be about 16.5, which was relatively acceptable value as published elsewhere. It can be concluded that the PAN precursor fibers were successfully produce in the solvent-free coagulalion process which possessed competitive mechanical properties.
first_indexed 2025-11-15T20:51:56Z
format Conference or Workshop Item
id utm-5464
institution Universiti Teknologi Malaysia
institution_category Local University
language English
last_indexed 2025-11-15T20:51:56Z
publishDate 2006
recordtype eprints
repository_type Digital Repository
spelling utm-54642010-06-01T15:31:05Z http://eprints.utm.my/5464/ On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process Ismail, Ahmad Fauzi Rahman, M. A. Mustafa, A. T Technology (General) The objective of this research is to investigate the appropriate range of coagulation bath temperature and polymer solution composition for spinning process in the solvent-free coagulation process and the effect of these parameters on carbon fibers precursor. The fabrication of the precursor fiber in the solvent-free coagulation process was carried out it a low residence time. The precursor fibers with excellent axial orientation and less number of micro-pores possess superior mechanical properties and enhance the performance of resulting carbon fibers. In the first stage of this study, the PAN polymer solution was prepared with incorporation of acrylamide as an additive. Th PAN/AM fibers were produced using a simple dry-wet spinning process. The PAN/AM fibers were then subjected to the oxidation process at 250 C in an oxygen-containing- atmosphere before underwent the carbonization process at 1000 °C. Through these studies, that a semi-dilute solution (18 wt.%) was found to be the most suitable polymer composition for the PAN/AM fibers fabrication at room temperature. It eased the fabrication process and produced the PAN/AM fibers with better mechanical properties. The PAN/AM fibers produced at coagulation bath temperature of 13 °C exhibited the excellent mechanical properties. At the coagulation bath temperature of 13 °C, the inward diffusion of non-solvent was still slow and consequendy reduced the number of micro-pores and fit for the drawing process. The ratio of carbon fiber to precursor modulus (Ec/Ep) was calculated to be about 16.5, which was relatively acceptable value as published elsewhere. It can be concluded that the PAN precursor fibers were successfully produce in the solvent-free coagulalion process which possessed competitive mechanical properties. 2006 Conference or Workshop Item PeerReviewed application/pdf en http://eprints.utm.my/5464/1/A.F.Ismail2006_OnTheFabricationAndCharacteristicsOfPAN.pdf Ismail, Ahmad Fauzi and Rahman, M. A. and Mustafa, A. (2006) On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process. In: 2nd National Carbon Fiber Conference 2006, 6th-9th June 2006, The City Bayview Hotel, Langkawi.
spellingShingle T Technology (General)
Ismail, Ahmad Fauzi
Rahman, M. A.
Mustafa, A.
On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process
title On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process
title_full On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process
title_fullStr On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process
title_full_unstemmed On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process
title_short On the fabrication and characteristics of PAN precursor fiber in the solvent-free coagulation process
title_sort on the fabrication and characteristics of pan precursor fiber in the solvent-free coagulation process
topic T Technology (General)
url http://eprints.utm.my/5464/
http://eprints.utm.my/5464/1/A.F.Ismail2006_OnTheFabricationAndCharacteristicsOfPAN.pdf