The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy

Problem Statement: Co-Cr based alloys which is well known for its high Young’s modulus, fatigue strength, wear resistance and corrosion resistance is an important metallic bio�material. However, till date there are only two type of Co-Cr alloy which are the castable and wrought cobalt alloy. Powd...

Full description

Bibliographic Details
Main Authors: Kamardan, M.Ghazali, A. Zaidi, N. Hidayah, Dalimin, M. Noh, A. Zaidi, A. Mujahid, Jamaludin, S. Bahrin, A.Jamil, M.Mahadi
Format: Article
Language:English
Published: Science Publications 2010
Subjects:
Online Access:http://eprints.uthm.edu.my/7837/
http://eprints.uthm.edu.my/7837/1/J4275_ee93d599874ea9274d1c5a19f7c1b27a.pdf
_version_ 1848889220419026944
author Kamardan, M.Ghazali
A. Zaidi, N. Hidayah
Dalimin, M. Noh
A. Zaidi, A. Mujahid
Jamaludin, S. Bahrin
A.Jamil, M.Mahadi
author_facet Kamardan, M.Ghazali
A. Zaidi, N. Hidayah
Dalimin, M. Noh
A. Zaidi, A. Mujahid
Jamaludin, S. Bahrin
A.Jamil, M.Mahadi
author_sort Kamardan, M.Ghazali
building UTHM Institutional Repository
collection Online Access
description Problem Statement: Co-Cr based alloys which is well known for its high Young’s modulus, fatigue strength, wear resistance and corrosion resistance is an important metallic bio�material. However, till date there are only two type of Co-Cr alloy which are the castable and wrought cobalt alloy. Powder Metallurgy route for cobalt is expected to give better result of Co-Cr alloy. The purpose of this research was mainly to study the sintering temperature effect to the shrinkage behavior of Cobalt Chromium (Co-Cr) alloy of the powder metallurgy route. Approach: Co-Cr was produced following P/M route under sintering temperature of 1000, 1100, 1200, 1300 and 1400oC. The sintering time was fixed at 60 min. Several tests has been conducted to determine this effect such as the rate of shrinkage measurement, the bulk density and porosity percentage measurement, compression and hardness tests and micro structural study. Result: From the study, it was found that the sintering temperature has caused the shrinkage of Co-Cr. The increasing of the sintering temperature has caused to the increasing of shrinkage of Co-Cr. This has resulted to the reduction of the pore volume and hence increased it density. In conjunction to that, the strength and the hardness of Co-Cr was increased. Conclusion: Therefore, it is hope that it will bring new view of powder metallurgy Co-Cr alloy as bio-material.
first_indexed 2025-11-15T20:22:43Z
format Article
id uthm-7837
institution Universiti Tun Hussein Onn Malaysia
institution_category Local University
language English
last_indexed 2025-11-15T20:22:43Z
publishDate 2010
publisher Science Publications
recordtype eprints
repository_type Digital Repository
spelling uthm-78372022-10-12T03:11:36Z http://eprints.uthm.edu.my/7837/ The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy Kamardan, M.Ghazali A. Zaidi, N. Hidayah Dalimin, M. Noh A. Zaidi, A. Mujahid Jamaludin, S. Bahrin A.Jamil, M.Mahadi T Technology (General) Problem Statement: Co-Cr based alloys which is well known for its high Young’s modulus, fatigue strength, wear resistance and corrosion resistance is an important metallic bio�material. However, till date there are only two type of Co-Cr alloy which are the castable and wrought cobalt alloy. Powder Metallurgy route for cobalt is expected to give better result of Co-Cr alloy. The purpose of this research was mainly to study the sintering temperature effect to the shrinkage behavior of Cobalt Chromium (Co-Cr) alloy of the powder metallurgy route. Approach: Co-Cr was produced following P/M route under sintering temperature of 1000, 1100, 1200, 1300 and 1400oC. The sintering time was fixed at 60 min. Several tests has been conducted to determine this effect such as the rate of shrinkage measurement, the bulk density and porosity percentage measurement, compression and hardness tests and micro structural study. Result: From the study, it was found that the sintering temperature has caused the shrinkage of Co-Cr. The increasing of the sintering temperature has caused to the increasing of shrinkage of Co-Cr. This has resulted to the reduction of the pore volume and hence increased it density. In conjunction to that, the strength and the hardness of Co-Cr was increased. Conclusion: Therefore, it is hope that it will bring new view of powder metallurgy Co-Cr alloy as bio-material. Science Publications 2010 Article PeerReviewed text en http://eprints.uthm.edu.my/7837/1/J4275_ee93d599874ea9274d1c5a19f7c1b27a.pdf Kamardan, M.Ghazali and A. Zaidi, N. Hidayah and Dalimin, M. Noh and A. Zaidi, A. Mujahid and Jamaludin, S. Bahrin and A.Jamil, M.Mahadi (2010) The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy. American Journal of Applied Sciences, 7 (11). pp. 1443-148.
spellingShingle T Technology (General)
Kamardan, M.Ghazali
A. Zaidi, N. Hidayah
Dalimin, M. Noh
A. Zaidi, A. Mujahid
Jamaludin, S. Bahrin
A.Jamil, M.Mahadi
The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy
title The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy
title_full The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy
title_fullStr The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy
title_full_unstemmed The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy
title_short The sintering temperature effect on the shrinkage behavior of cobalt chromium alloy
title_sort sintering temperature effect on the shrinkage behavior of cobalt chromium alloy
topic T Technology (General)
url http://eprints.uthm.edu.my/7837/
http://eprints.uthm.edu.my/7837/1/J4275_ee93d599874ea9274d1c5a19f7c1b27a.pdf