Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode
This paper presents the fabrication and thickness analysis of TiO2 on Fluorine-doped Tin Oxide (FTO) glass for Dye-Sensitized Solar Cell (DSSC). The TiO2 layer was deposited on the cleaned FTO glass using doctor blade technique and the thickness of the TiO2 were controlled by with different layers o...
| Main Authors: | , , , , , , , |
|---|---|
| Format: | Conference or Workshop Item |
| Language: | English |
| Published: |
IEEE
2019
|
| Online Access: | http://psasir.upm.edu.my/id/eprint/78092/ http://psasir.upm.edu.my/id/eprint/78092/1/Efficiency%20performance%20effect%20of%20TiO2%20thickness%20deposited%20on%20FTO%20coated%20glass%20photoanode.pdf |
| _version_ | 1848858410993319936 |
|---|---|
| author | Shaban, Suraya Shafie, Suhaidi Mustafa, Mohd Amrallah Sudhir, Pandey Shyam Ahmad, Fauzan Hamidon, Mohd Nizar Lokman, Muhammad Quisar Mohamed Sharif, Noor Fadzilah |
| author_facet | Shaban, Suraya Shafie, Suhaidi Mustafa, Mohd Amrallah Sudhir, Pandey Shyam Ahmad, Fauzan Hamidon, Mohd Nizar Lokman, Muhammad Quisar Mohamed Sharif, Noor Fadzilah |
| author_sort | Shaban, Suraya |
| building | UPM Institutional Repository |
| collection | Online Access |
| description | This paper presents the fabrication and thickness analysis of TiO2 on Fluorine-doped Tin Oxide (FTO) glass for Dye-Sensitized Solar Cell (DSSC). The TiO2 layer was deposited on the cleaned FTO glass using doctor blade technique and the thickness of the TiO2 were controlled by with different layers of adhesive tape. This results showed that the two-layer with thickness 15.09 μm of adhesive tape achieved the highest efficiency of 4.73 %, and followed by three-layer and one-layer at 3.64% at 2.32 % respectively. |
| first_indexed | 2025-11-15T12:13:01Z |
| format | Conference or Workshop Item |
| id | upm-78092 |
| institution | Universiti Putra Malaysia |
| institution_category | Local University |
| language | English |
| last_indexed | 2025-11-15T12:13:01Z |
| publishDate | 2019 |
| publisher | IEEE |
| recordtype | eprints |
| repository_type | Digital Repository |
| spelling | upm-780922020-06-03T06:31:10Z http://psasir.upm.edu.my/id/eprint/78092/ Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode Shaban, Suraya Shafie, Suhaidi Mustafa, Mohd Amrallah Sudhir, Pandey Shyam Ahmad, Fauzan Hamidon, Mohd Nizar Lokman, Muhammad Quisar Mohamed Sharif, Noor Fadzilah This paper presents the fabrication and thickness analysis of TiO2 on Fluorine-doped Tin Oxide (FTO) glass for Dye-Sensitized Solar Cell (DSSC). The TiO2 layer was deposited on the cleaned FTO glass using doctor blade technique and the thickness of the TiO2 were controlled by with different layers of adhesive tape. This results showed that the two-layer with thickness 15.09 μm of adhesive tape achieved the highest efficiency of 4.73 %, and followed by three-layer and one-layer at 3.64% at 2.32 % respectively. IEEE 2019 Conference or Workshop Item PeerReviewed text en http://psasir.upm.edu.my/id/eprint/78092/1/Efficiency%20performance%20effect%20of%20TiO2%20thickness%20deposited%20on%20FTO%20coated%20glass%20photoanode.pdf Shaban, Suraya and Shafie, Suhaidi and Mustafa, Mohd Amrallah and Sudhir, Pandey Shyam and Ahmad, Fauzan and Hamidon, Mohd Nizar and Lokman, Muhammad Quisar and Mohamed Sharif, Noor Fadzilah (2019) Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode. In: 2019 4th IEEE International Circuit and System Symposium (ICSyS), 18-19 Sept. 2019, Hotel Istana, Kuala Lumpur, Malaysia. (pp. 1-4). 10.1109/ICSyS47076.2019.8982538 |
| spellingShingle | Shaban, Suraya Shafie, Suhaidi Mustafa, Mohd Amrallah Sudhir, Pandey Shyam Ahmad, Fauzan Hamidon, Mohd Nizar Lokman, Muhammad Quisar Mohamed Sharif, Noor Fadzilah Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode |
| title | Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode |
| title_full | Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode |
| title_fullStr | Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode |
| title_full_unstemmed | Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode |
| title_short | Efficiency performance effect of TiO2 thickness deposited on FTO coated glass photoanode |
| title_sort | efficiency performance effect of tio2 thickness deposited on fto coated glass photoanode |
| url | http://psasir.upm.edu.my/id/eprint/78092/ http://psasir.upm.edu.my/id/eprint/78092/ http://psasir.upm.edu.my/id/eprint/78092/1/Efficiency%20performance%20effect%20of%20TiO2%20thickness%20deposited%20on%20FTO%20coated%20glass%20photoanode.pdf |