The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2

Photopyroelectric spectroscopy is used to study the variation of optical absorption of the ceramic xMn02 - 0.4 Bi2O3 - 0.4 TiO2 - ZnO, x = 0, 0.4 mol% sintered for 1-4 hours at the isothermal temperature, 1220°C. The wavelength of incident light, modulated at 12 Hz, is kept in the range 310 to 810 n...

Full description

Bibliographic Details
Main Authors: Rizwan, Zahid, Zakaria, Azmi
Format: Conference or Workshop Item
Language:English
Published: IEEE 2008
Online Access:http://psasir.upm.edu.my/id/eprint/37569/
http://psasir.upm.edu.my/id/eprint/37569/1/The%20variation%20of%20optical%20absorption%20edge%20with%20sintering%20time%20for%20the%20ceramic%20ZnO%20%2B%20xMnO2-Bi2O3-TiO2.pdf
_version_ 1848848642322989056
author Rizwan, Zahid
Zakaria, Azmi
author_facet Rizwan, Zahid
Zakaria, Azmi
author_sort Rizwan, Zahid
building UPM Institutional Repository
collection Online Access
description Photopyroelectric spectroscopy is used to study the variation of optical absorption of the ceramic xMn02 - 0.4 Bi2O3 - 0.4 TiO2 - ZnO, x = 0, 0.4 mol% sintered for 1-4 hours at the isothermal temperature, 1220°C. The wavelength of incident light, modulated at 12 Hz, is kept in the range 310 to 810 nm. The band-gap energy is reduced from 3.2 eV (for pure ZnO) to 2.83 eV for 0 mol% MnO2 for 1 hour sintering time and decreases further with the further increase of sintering time. Eg is decreased to 2.39 eV for 1 hour sintering time after the addition of 0.4 mol% of MnO2 in the ceramic combination. It is reduced to a value 1.9 eV with the further increase of sintering time. The variation of steepness factor σA and σB which characterizes the slop of exponential optical absorption, is correlated with the variation of Eg, sintering time and doping of MnO2. Microstructure and compositional analysis of the selected areas are analyzed using SEM and EDAX.
first_indexed 2025-11-15T09:37:45Z
format Conference or Workshop Item
id upm-37569
institution Universiti Putra Malaysia
institution_category Local University
language English
last_indexed 2025-11-15T09:37:45Z
publishDate 2008
publisher IEEE
recordtype eprints
repository_type Digital Repository
spelling upm-375692020-08-10T02:23:56Z http://psasir.upm.edu.my/id/eprint/37569/ The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2 Rizwan, Zahid Zakaria, Azmi Photopyroelectric spectroscopy is used to study the variation of optical absorption of the ceramic xMn02 - 0.4 Bi2O3 - 0.4 TiO2 - ZnO, x = 0, 0.4 mol% sintered for 1-4 hours at the isothermal temperature, 1220°C. The wavelength of incident light, modulated at 12 Hz, is kept in the range 310 to 810 nm. The band-gap energy is reduced from 3.2 eV (for pure ZnO) to 2.83 eV for 0 mol% MnO2 for 1 hour sintering time and decreases further with the further increase of sintering time. Eg is decreased to 2.39 eV for 1 hour sintering time after the addition of 0.4 mol% of MnO2 in the ceramic combination. It is reduced to a value 1.9 eV with the further increase of sintering time. The variation of steepness factor σA and σB which characterizes the slop of exponential optical absorption, is correlated with the variation of Eg, sintering time and doping of MnO2. Microstructure and compositional analysis of the selected areas are analyzed using SEM and EDAX. IEEE 2008 Conference or Workshop Item PeerReviewed text en http://psasir.upm.edu.my/id/eprint/37569/1/The%20variation%20of%20optical%20absorption%20edge%20with%20sintering%20time%20for%20the%20ceramic%20ZnO%20%2B%20xMnO2-Bi2O3-TiO2.pdf Rizwan, Zahid and Zakaria, Azmi (2008) The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2. In: 2008 IEEE International Conference on Semiconductor Electronics (ICSE 2008), 25-27 Nov. 2008, Johor Bahru, Malaysia. (pp. 541-544). 10.1109/SMELEC.2008.4770383
spellingShingle Rizwan, Zahid
Zakaria, Azmi
The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2
title The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2
title_full The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2
title_fullStr The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2
title_full_unstemmed The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2
title_short The variation of optical absorption edge with sintering time for the ceramic ZnO + xMnO2-Bi2O3-TiO2
title_sort variation of optical absorption edge with sintering time for the ceramic zno + xmno2-bi2o3-tio2
url http://psasir.upm.edu.my/id/eprint/37569/
http://psasir.upm.edu.my/id/eprint/37569/
http://psasir.upm.edu.my/id/eprint/37569/1/The%20variation%20of%20optical%20absorption%20edge%20with%20sintering%20time%20for%20the%20ceramic%20ZnO%20%2B%20xMnO2-Bi2O3-TiO2.pdf