Preliminary morphological studies on the effect of substitution in yttrium iron garnet system

This is a preliminary study on the phase and morphology of La-subtitution in Y3.0-XLaXFe5O12 prepared via conventional method with x = 0.0, 0.5, 1.0, 1.5, 2.0, 2.5 and 3.0. The Y3.0-XLaXFe5O12 series were sintered at 1300°c for 10 hours. XRD studies confirmed the garnet phase of all the samples. Pa...

Full description

Bibliographic Details
Main Authors: See, Alex, Yahya, Noorhana, Hashim, Mansor
Format: Conference or Workshop Item
Language:English
Published: Universiti Putra Malaysia Press 2005
Online Access:http://psasir.upm.edu.my/id/eprint/34009/
http://psasir.upm.edu.my/id/eprint/34009/1/34009.pdf
_version_ 1848847655076102144
author See, Alex
Yahya, Noorhana
Hashim, Mansor
author_facet See, Alex
Yahya, Noorhana
Hashim, Mansor
author_sort See, Alex
building UPM Institutional Repository
collection Online Access
description This is a preliminary study on the phase and morphology of La-subtitution in Y3.0-XLaXFe5O12 prepared via conventional method with x = 0.0, 0.5, 1.0, 1.5, 2.0, 2.5 and 3.0. The Y3.0-XLaXFe5O12 series were sintered at 1300°c for 10 hours. XRD studies confirmed the garnet phase of all the samples. Particle size distribution was done to study the effect of Lanthanum on the effect of the sample powder. From the result of this work, SEM analysis, the Y2.5La0.5Fe5O12 has the largest grain size (4.146). In conclusion, Lanthanum helps in constituting smaller grain size (1.852 μm) and better magnetic properties.
first_indexed 2025-11-15T09:22:03Z
format Conference or Workshop Item
id upm-34009
institution Universiti Putra Malaysia
institution_category Local University
language English
last_indexed 2025-11-15T09:22:03Z
publishDate 2005
publisher Universiti Putra Malaysia Press
recordtype eprints
repository_type Digital Repository
spelling upm-340092015-05-11T01:22:09Z http://psasir.upm.edu.my/id/eprint/34009/ Preliminary morphological studies on the effect of substitution in yttrium iron garnet system See, Alex Yahya, Noorhana Hashim, Mansor This is a preliminary study on the phase and morphology of La-subtitution in Y3.0-XLaXFe5O12 prepared via conventional method with x = 0.0, 0.5, 1.0, 1.5, 2.0, 2.5 and 3.0. The Y3.0-XLaXFe5O12 series were sintered at 1300°c for 10 hours. XRD studies confirmed the garnet phase of all the samples. Particle size distribution was done to study the effect of Lanthanum on the effect of the sample powder. From the result of this work, SEM analysis, the Y2.5La0.5Fe5O12 has the largest grain size (4.146). In conclusion, Lanthanum helps in constituting smaller grain size (1.852 μm) and better magnetic properties. Universiti Putra Malaysia Press 2005 Conference or Workshop Item NonPeerReviewed application/pdf en http://psasir.upm.edu.my/id/eprint/34009/1/34009.pdf See, Alex and Yahya, Noorhana and Hashim, Mansor (2005) Preliminary morphological studies on the effect of substitution in yttrium iron garnet system. In: International Advanced Technology Congress: Conference on Advanced Materials (CAM 2005), 6 - 8 Dec. 2005, Putrajaya, Malaysia. (pp. 623-629).
spellingShingle See, Alex
Yahya, Noorhana
Hashim, Mansor
Preliminary morphological studies on the effect of substitution in yttrium iron garnet system
title Preliminary morphological studies on the effect of substitution in yttrium iron garnet system
title_full Preliminary morphological studies on the effect of substitution in yttrium iron garnet system
title_fullStr Preliminary morphological studies on the effect of substitution in yttrium iron garnet system
title_full_unstemmed Preliminary morphological studies on the effect of substitution in yttrium iron garnet system
title_short Preliminary morphological studies on the effect of substitution in yttrium iron garnet system
title_sort preliminary morphological studies on the effect of substitution in yttrium iron garnet system
url http://psasir.upm.edu.my/id/eprint/34009/
http://psasir.upm.edu.my/id/eprint/34009/1/34009.pdf