Development of biocomposite wall cladding from kenaf fibre by extrusion molding process

Nowadays, natural fibre-thermoplastics composites (NFPC) are replacing the conventional wood and timber due to its lower cost, avoid deforestation, higher strength-to-weight ratio and resistant to termites. These composites can be utilized for non-structural components of a building system such as d...

Full description

Bibliographic Details
Main Authors: Abdan, Khalina, Zainudin, Edi Syams, Abdul Rahman, Mohd Faizal, Harun, Jalaluddin, Abdul Hanan, Umar, W. N., W. N. Syuhada
Format: Article
Language:English
Published: Trans Tech Publications 2011
Online Access:http://psasir.upm.edu.my/id/eprint/22931/
http://psasir.upm.edu.my/id/eprint/22931/1/Development%20of%20biocomposite%20wall%20cladding%20from%20kenaf%20fibre%20by%20extrusion%20molding%20process.pdf
_version_ 1848844618857185280
author Abdan, Khalina
Zainudin, Edi Syams
Abdul Rahman, Mohd Faizal
Harun, Jalaluddin
Abdul Hanan, Umar
W. N., W. N. Syuhada
author_facet Abdan, Khalina
Zainudin, Edi Syams
Abdul Rahman, Mohd Faizal
Harun, Jalaluddin
Abdul Hanan, Umar
W. N., W. N. Syuhada
author_sort Abdan, Khalina
building UPM Institutional Repository
collection Online Access
description Nowadays, natural fibre-thermoplastics composites (NFPC) are replacing the conventional wood and timber due to its lower cost, avoid deforestation, higher strength-to-weight ratio and resistant to termites. These composites can be utilized for non-structural components of a building system such as decking, wall cladding, floor tiles and window frame. A natural fiber/plastic composite was produced by extrusion molding process to create a wall cladding profile. The raw materials used for the composites are 40% kenaf fibre and 60% polypropylene (PP). These materials were compounded through a twin-screw extruder and then cut into pellets. The moisture content found in the kenaf/PP composites (KPC) pellets was 2.89%. Therefore, the pellets required to be oven dried every time right before entering the hopper of the extruder. The temperature along the barrel was set to 180°C and the die head temperature is set to 165°C. At the end of the extrusion molding process, pressurized air was used for cooling the profile. Then, samples of the wall cladding were taken back to the laboratory for product quality assurance. Measurements of the samples show that the product experiences 3% of shrinkage in term of width and 1% of shrinkage in term of thickness. Water absorption test indicates an increase of 13.6% of weight after 24 hours immersion of water. Impact strength test was also conducted on the wall cladding samples and the mean result was 2.55 kJ/m 2 Tensile test on the extruded KPC product indicates a low tensile strength at 4.51 MPa and tensile modulus of 205.01 MPa. The sample also proven to be light weight as the density of the material was found to be 0.618g/cm 3.
first_indexed 2025-11-15T08:33:47Z
format Article
id upm-22931
institution Universiti Putra Malaysia
institution_category Local University
language English
last_indexed 2025-11-15T08:33:47Z
publishDate 2011
publisher Trans Tech Publications
recordtype eprints
repository_type Digital Repository
spelling upm-229312015-12-01T02:23:48Z http://psasir.upm.edu.my/id/eprint/22931/ Development of biocomposite wall cladding from kenaf fibre by extrusion molding process Abdan, Khalina Zainudin, Edi Syams Abdul Rahman, Mohd Faizal Harun, Jalaluddin Abdul Hanan, Umar W. N., W. N. Syuhada Nowadays, natural fibre-thermoplastics composites (NFPC) are replacing the conventional wood and timber due to its lower cost, avoid deforestation, higher strength-to-weight ratio and resistant to termites. These composites can be utilized for non-structural components of a building system such as decking, wall cladding, floor tiles and window frame. A natural fiber/plastic composite was produced by extrusion molding process to create a wall cladding profile. The raw materials used for the composites are 40% kenaf fibre and 60% polypropylene (PP). These materials were compounded through a twin-screw extruder and then cut into pellets. The moisture content found in the kenaf/PP composites (KPC) pellets was 2.89%. Therefore, the pellets required to be oven dried every time right before entering the hopper of the extruder. The temperature along the barrel was set to 180°C and the die head temperature is set to 165°C. At the end of the extrusion molding process, pressurized air was used for cooling the profile. Then, samples of the wall cladding were taken back to the laboratory for product quality assurance. Measurements of the samples show that the product experiences 3% of shrinkage in term of width and 1% of shrinkage in term of thickness. Water absorption test indicates an increase of 13.6% of weight after 24 hours immersion of water. Impact strength test was also conducted on the wall cladding samples and the mean result was 2.55 kJ/m 2 Tensile test on the extruded KPC product indicates a low tensile strength at 4.51 MPa and tensile modulus of 205.01 MPa. The sample also proven to be light weight as the density of the material was found to be 0.618g/cm 3. Trans Tech Publications 2011 Article PeerReviewed application/pdf en http://psasir.upm.edu.my/id/eprint/22931/1/Development%20of%20biocomposite%20wall%20cladding%20from%20kenaf%20fibre%20by%20extrusion%20molding%20process.pdf Abdan, Khalina and Zainudin, Edi Syams and Abdul Rahman, Mohd Faizal and Harun, Jalaluddin and Abdul Hanan, Umar and W. N., W. N. Syuhada (2011) Development of biocomposite wall cladding from kenaf fibre by extrusion molding process. Key Engineering Materials, 471-472. pp. 239-244. ISSN 1013-9826; ESSN: 1662-9795 http://www.scientific.net/KEM.471-472.239 10.4028/www.scientific.net/KEM.471-472.239
spellingShingle Abdan, Khalina
Zainudin, Edi Syams
Abdul Rahman, Mohd Faizal
Harun, Jalaluddin
Abdul Hanan, Umar
W. N., W. N. Syuhada
Development of biocomposite wall cladding from kenaf fibre by extrusion molding process
title Development of biocomposite wall cladding from kenaf fibre by extrusion molding process
title_full Development of biocomposite wall cladding from kenaf fibre by extrusion molding process
title_fullStr Development of biocomposite wall cladding from kenaf fibre by extrusion molding process
title_full_unstemmed Development of biocomposite wall cladding from kenaf fibre by extrusion molding process
title_short Development of biocomposite wall cladding from kenaf fibre by extrusion molding process
title_sort development of biocomposite wall cladding from kenaf fibre by extrusion molding process
url http://psasir.upm.edu.my/id/eprint/22931/
http://psasir.upm.edu.my/id/eprint/22931/
http://psasir.upm.edu.my/id/eprint/22931/
http://psasir.upm.edu.my/id/eprint/22931/1/Development%20of%20biocomposite%20wall%20cladding%20from%20kenaf%20fibre%20by%20extrusion%20molding%20process.pdf