Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz

This research was designed to form better dielectric composite material using one steady state dielectric (mullite) with a good dielectric material (strontium titanate). Distinct dielectric composites were successfully produced using locally sourced kaolinite clay. The samples were made using mullit...

Full description

Bibliographic Details
Main Authors: See, Alex, Hassan, Jumiah, Hashim, Mansor, Shaari, Abdul Halim, Wan Yusoff, Wan Mohamad Daud
Format: Article
Language:English
Published: Malaysian Solid State Science and Technology Society 2009
Online Access:http://psasir.upm.edu.my/id/eprint/14052/
http://psasir.upm.edu.my/id/eprint/14052/1/Dielectric%20properties%20of%20strontium%20titanate%20filled%20mullite%20composites%20at%2010%20Hz%20-%201%20MHz.pdf
_version_ 1848842286398439424
author See, Alex
Hassan, Jumiah
Hashim, Mansor
Shaari, Abdul Halim
Wan Yusoff, Wan Mohamad Daud
author_facet See, Alex
Hassan, Jumiah
Hashim, Mansor
Shaari, Abdul Halim
Wan Yusoff, Wan Mohamad Daud
author_sort See, Alex
building UPM Institutional Repository
collection Online Access
description This research was designed to form better dielectric composite material using one steady state dielectric (mullite) with a good dielectric material (strontium titanate). Distinct dielectric composites were successfully produced using locally sourced kaolinite clay. The samples were made using mullite as the base matrix and strontium titanate (ST) added at varying ratios. Strontium titanate was synthesized via solid-state reaction using strontium carbonate and rutile titanium (IV) oxide sintered at 1300°C. Local white kaolinite was used to fuse the strontium titanate material at varying weight ratios. The powders were dry-mixed and made into pellets for calcination at 1000°C. XRD and SEM characterizations were made. The dielectric measurements were carried out using the HP 4192A LF Impedance Analyzer dielectric setup in the frequency range of 10 Hz to 1 MHz. Three samples were prepared, namely ST 60%, ST 70% and ST 80%. The dielectric measurements were carried out in a controlled LT furnace at 30°C - 400°C. Measurements showed distinct varying interfacial encapsulation and dipolar relaxation for all composite samples.
first_indexed 2025-11-15T07:56:43Z
format Article
id upm-14052
institution Universiti Putra Malaysia
institution_category Local University
language English
last_indexed 2025-11-15T07:56:43Z
publishDate 2009
publisher Malaysian Solid State Science and Technology Society
recordtype eprints
repository_type Digital Repository
spelling upm-140522018-09-04T07:59:29Z http://psasir.upm.edu.my/id/eprint/14052/ Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz See, Alex Hassan, Jumiah Hashim, Mansor Shaari, Abdul Halim Wan Yusoff, Wan Mohamad Daud This research was designed to form better dielectric composite material using one steady state dielectric (mullite) with a good dielectric material (strontium titanate). Distinct dielectric composites were successfully produced using locally sourced kaolinite clay. The samples were made using mullite as the base matrix and strontium titanate (ST) added at varying ratios. Strontium titanate was synthesized via solid-state reaction using strontium carbonate and rutile titanium (IV) oxide sintered at 1300°C. Local white kaolinite was used to fuse the strontium titanate material at varying weight ratios. The powders were dry-mixed and made into pellets for calcination at 1000°C. XRD and SEM characterizations were made. The dielectric measurements were carried out using the HP 4192A LF Impedance Analyzer dielectric setup in the frequency range of 10 Hz to 1 MHz. Three samples were prepared, namely ST 60%, ST 70% and ST 80%. The dielectric measurements were carried out in a controlled LT furnace at 30°C - 400°C. Measurements showed distinct varying interfacial encapsulation and dipolar relaxation for all composite samples. Malaysian Solid State Science and Technology Society 2009 Article PeerReviewed text en http://psasir.upm.edu.my/id/eprint/14052/1/Dielectric%20properties%20of%20strontium%20titanate%20filled%20mullite%20composites%20at%2010%20Hz%20-%201%20MHz.pdf See, Alex and Hassan, Jumiah and Hashim, Mansor and Shaari, Abdul Halim and Wan Yusoff, Wan Mohamad Daud (2009) Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz. Solid State Science and Technology, 17 (2). pp. 182-188. ISSN 0128-7389 http://journal.masshp.net/volume-17-no-2-2009/
spellingShingle See, Alex
Hassan, Jumiah
Hashim, Mansor
Shaari, Abdul Halim
Wan Yusoff, Wan Mohamad Daud
Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz
title Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz
title_full Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz
title_fullStr Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz
title_full_unstemmed Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz
title_short Dielectric properties of strontium titanate filled mullite composites at 10 Hz - 1 MHz
title_sort dielectric properties of strontium titanate filled mullite composites at 10 hz - 1 mhz
url http://psasir.upm.edu.my/id/eprint/14052/
http://psasir.upm.edu.my/id/eprint/14052/
http://psasir.upm.edu.my/id/eprint/14052/1/Dielectric%20properties%20of%20strontium%20titanate%20filled%20mullite%20composites%20at%2010%20Hz%20-%201%20MHz.pdf