Dielectric characterization of thermoplastic natural rubber/strontium titanate composites at 10 Hz to 1 MHz

The dielectric properties of Thermoplastic Natural Rubber (TPNR)/Strontium Titanate (SrTiO3) composites was determined at room temperature, 27oC using the Impedance Analyzer at frequencies 10 Hz to 1 MHz. TPNR is formed as the matrix while SrTiO3 acts as the filler. Six samples were prepared at perc...

Full description

Bibliographic Details
Main Authors: Hassan, Jumiah, Rajaram, Deventharan, Hashim, Mansor, Ahmad, Azizan, Abbas, Zulkifly
Format: Article
Language:English
Published: Malaysian Institute of Physics 2008
Online Access:http://psasir.upm.edu.my/id/eprint/14045/
http://psasir.upm.edu.my/id/eprint/14045/1/Dielectric%20characterization%20of%20thermoplastic%20natural%20rubber.pdf
Description
Summary:The dielectric properties of Thermoplastic Natural Rubber (TPNR)/Strontium Titanate (SrTiO3) composites was determined at room temperature, 27oC using the Impedance Analyzer at frequencies 10 Hz to 1 MHz. TPNR is formed as the matrix while SrTiO3 acts as the filler. Six samples were prepared at percentages of fillers from 0 to 50% at 10% intervals. The results indicate that the dielectric constant is almost independent of frequency from 100 Hz to 1 MHz, but the dielectric loss factor decreased with increasing frequency. This could probably be due to interfacial polarization and ionic losses. The dielectric properties are also affected by the composition of the filler, SrTiO3.