Effect of banana skins filler on thermal behavior of natural rubber latex films

This study is done to produce latex film with 0 %, 5 %, 10 %, 15 % and 20 % banana skins as filler and to investigate the effect of banana skin on thermal behavior of natural rubber latex films. Banana skin contains a lot of minerals, sugar, starch, protein and so on. The bio-based material such a...

Full description

Bibliographic Details
Main Author: Low, Miao Ying
Format: Undergraduates Project Papers
Language:English
Published: 2012
Subjects:
Online Access:http://umpir.ump.edu.my/id/eprint/7796/
http://umpir.ump.edu.my/id/eprint/7796/1/LOW_MIAO_YING.PDF
_version_ 1848818089755410432
author Low, Miao Ying
author_facet Low, Miao Ying
author_sort Low, Miao Ying
building UMP Institutional Repository
collection Online Access
description This study is done to produce latex film with 0 %, 5 %, 10 %, 15 % and 20 % banana skins as filler and to investigate the effect of banana skin on thermal behavior of natural rubber latex films. Banana skin contains a lot of minerals, sugar, starch, protein and so on. The bio-based material such as starch is widely use in latex industries to produce of biodegradable plastic and in the production of latex glove due to its properties. In terms of industrial application, thermal performance of rubber is the key importance since in the production of rubber based products processing temperature are usually high and close to their degradation temperature. Banana skin is dried by using drying cabinet at 40 °C until fully dried and followed by grinding process by using grinder to get banana skin powder. Sieving process is necessary to produce fine banana skin powder before dissolve it into distilled water. Effect of different banana loading on natural rubber latex films are investigated after vulcanization process and dipping process. Thermal properties of the natural rubber latex which filled with banana skin powder are determined by using Mettler Toledo Thermagravimetric Analyzer/Differential Scanning Calorimeter (TGA/DSC). It can evaluate the thermal stability such as weight loss, rate of degradation and also heat flow. Finally, observation for microscopic behavior on surface of films will carry out by using Scanning Electron Microscope (SEM). This is to study the dispersion of different banana loading on the natural rubber latex films. There are no significant difference in term of thermal stability of pure natural rubber latex film and natural rubber latex with filler. Therefore by adding banana skin powder into natural rubber latex is potentially to apply in latex based product industry.
first_indexed 2025-11-15T01:32:07Z
format Undergraduates Project Papers
id ump-7796
institution Universiti Malaysia Pahang
institution_category Local University
language English
last_indexed 2025-11-15T01:32:07Z
publishDate 2012
recordtype eprints
repository_type Digital Repository
spelling ump-77962021-06-09T03:21:26Z http://umpir.ump.edu.my/id/eprint/7796/ Effect of banana skins filler on thermal behavior of natural rubber latex films Low, Miao Ying QK Botany This study is done to produce latex film with 0 %, 5 %, 10 %, 15 % and 20 % banana skins as filler and to investigate the effect of banana skin on thermal behavior of natural rubber latex films. Banana skin contains a lot of minerals, sugar, starch, protein and so on. The bio-based material such as starch is widely use in latex industries to produce of biodegradable plastic and in the production of latex glove due to its properties. In terms of industrial application, thermal performance of rubber is the key importance since in the production of rubber based products processing temperature are usually high and close to their degradation temperature. Banana skin is dried by using drying cabinet at 40 °C until fully dried and followed by grinding process by using grinder to get banana skin powder. Sieving process is necessary to produce fine banana skin powder before dissolve it into distilled water. Effect of different banana loading on natural rubber latex films are investigated after vulcanization process and dipping process. Thermal properties of the natural rubber latex which filled with banana skin powder are determined by using Mettler Toledo Thermagravimetric Analyzer/Differential Scanning Calorimeter (TGA/DSC). It can evaluate the thermal stability such as weight loss, rate of degradation and also heat flow. Finally, observation for microscopic behavior on surface of films will carry out by using Scanning Electron Microscope (SEM). This is to study the dispersion of different banana loading on the natural rubber latex films. There are no significant difference in term of thermal stability of pure natural rubber latex film and natural rubber latex with filler. Therefore by adding banana skin powder into natural rubber latex is potentially to apply in latex based product industry. 2012 Undergraduates Project Papers NonPeerReviewed application/pdf en http://umpir.ump.edu.my/id/eprint/7796/1/LOW_MIAO_YING.PDF Low, Miao Ying (2012) Effect of banana skins filler on thermal behavior of natural rubber latex films. Faculty of Industrial Sciences & Technology, Universiti Malaysia Pahang.
spellingShingle QK Botany
Low, Miao Ying
Effect of banana skins filler on thermal behavior of natural rubber latex films
title Effect of banana skins filler on thermal behavior of natural rubber latex films
title_full Effect of banana skins filler on thermal behavior of natural rubber latex films
title_fullStr Effect of banana skins filler on thermal behavior of natural rubber latex films
title_full_unstemmed Effect of banana skins filler on thermal behavior of natural rubber latex films
title_short Effect of banana skins filler on thermal behavior of natural rubber latex films
title_sort effect of banana skins filler on thermal behavior of natural rubber latex films
topic QK Botany
url http://umpir.ump.edu.my/id/eprint/7796/
http://umpir.ump.edu.my/id/eprint/7796/1/LOW_MIAO_YING.PDF