Preparation of Zn0.6Cd0.4o nanorods and its characterization
Hexagonal nanorods of Zn0.6Cd0.4O thin films were synthesized by electrodeposition technique using 0.6% of ZnCl2 and 0.4% of CdCl2 electrolytes. The synthesized Zn0.6Cd0.4O nanorods have uniform hexagonal crystallographic planes, and their diameters are about 100 nm. The ultra-violet (UV) near-band-...
| Main Authors: | , , |
|---|---|
| Format: | Proceeding Paper |
| Language: | English English English English |
| Published: |
2013
|
| Subjects: | |
| Online Access: | http://irep.iium.edu.my/36138/ http://irep.iium.edu.my/36138/1/Camera_Ready.pdf http://irep.iium.edu.my/36138/4/1099_Acceptance_%28Included%29.pdf http://irep.iium.edu.my/36138/5/Certificate_of_Participation_%28ID_1099%29.pdf http://irep.iium.edu.my/36138/9/ICBioE2013.pdf |
| _version_ | 1848781169029545984 |
|---|---|
| author | Mohamad, Souad A. Othman, Raihan Mushtaq, Umer |
| author_facet | Mohamad, Souad A. Othman, Raihan Mushtaq, Umer |
| author_sort | Mohamad, Souad A. |
| building | IIUM Repository |
| collection | Online Access |
| description | Hexagonal nanorods of Zn0.6Cd0.4O thin films were synthesized by electrodeposition technique using 0.6% of ZnCl2 and 0.4% of CdCl2 electrolytes. The synthesized Zn0.6Cd0.4O nanorods have uniform hexagonal crystallographic planes, and their diameters are about 100 nm. The ultra-violet (UV) near-band-edge (NBE) emission was red-shifted from 2.75 eV to 3.02 eV due to the direct tailoring of band gap caused by Cd/Zn substitution. The FESEM images of Zn0.6Cd0.4O confirms that hexagonal nanorods were first time synthesized via electrodeposition technique at temperature of 90 oC and the size of each regular face of hexagonal nanorods is about 63.6 nm. The characterizations for Zn0.6Cd0.4O were analyzed and the temperature is a key parameter for the formation of different morphologies of Zn0.6Cd0.4O nanostructures. |
| first_indexed | 2025-11-14T15:45:17Z |
| format | Proceeding Paper |
| id | iium-36138 |
| institution | International Islamic University Malaysia |
| institution_category | Local University |
| language | English English English English |
| last_indexed | 2025-11-14T15:45:17Z |
| publishDate | 2013 |
| recordtype | eprints |
| repository_type | Digital Repository |
| spelling | iium-361382015-01-27T06:39:02Z http://irep.iium.edu.my/36138/ Preparation of Zn0.6Cd0.4o nanorods and its characterization Mohamad, Souad A. Othman, Raihan Mushtaq, Umer T175 Industrial research. Research and development Hexagonal nanorods of Zn0.6Cd0.4O thin films were synthesized by electrodeposition technique using 0.6% of ZnCl2 and 0.4% of CdCl2 electrolytes. The synthesized Zn0.6Cd0.4O nanorods have uniform hexagonal crystallographic planes, and their diameters are about 100 nm. The ultra-violet (UV) near-band-edge (NBE) emission was red-shifted from 2.75 eV to 3.02 eV due to the direct tailoring of band gap caused by Cd/Zn substitution. The FESEM images of Zn0.6Cd0.4O confirms that hexagonal nanorods were first time synthesized via electrodeposition technique at temperature of 90 oC and the size of each regular face of hexagonal nanorods is about 63.6 nm. The characterizations for Zn0.6Cd0.4O were analyzed and the temperature is a key parameter for the formation of different morphologies of Zn0.6Cd0.4O nanostructures. 2013-07-02 Proceeding Paper NonPeerReviewed application/pdf en http://irep.iium.edu.my/36138/1/Camera_Ready.pdf application/pdf en http://irep.iium.edu.my/36138/4/1099_Acceptance_%28Included%29.pdf application/pdf en http://irep.iium.edu.my/36138/5/Certificate_of_Participation_%28ID_1099%29.pdf application/pdf en http://irep.iium.edu.my/36138/9/ICBioE2013.pdf Mohamad, Souad A. and Othman, Raihan and Mushtaq, Umer (2013) Preparation of Zn0.6Cd0.4o nanorods and its characterization. In: Third International Conference on Biotechnology (ICBIoE 2013), 2nd - 4th July 2013 , Berjaya Times Square Hotel, Kuala Lumpur. (Unpublished) http://www.iium.edu.my/icbioe/2013/ |
| spellingShingle | T175 Industrial research. Research and development Mohamad, Souad A. Othman, Raihan Mushtaq, Umer Preparation of Zn0.6Cd0.4o nanorods and its characterization |
| title | Preparation of Zn0.6Cd0.4o nanorods and its characterization |
| title_full | Preparation of Zn0.6Cd0.4o nanorods and its characterization |
| title_fullStr | Preparation of Zn0.6Cd0.4o nanorods and its characterization |
| title_full_unstemmed | Preparation of Zn0.6Cd0.4o nanorods and its characterization |
| title_short | Preparation of Zn0.6Cd0.4o nanorods and its characterization |
| title_sort | preparation of zn0.6cd0.4o nanorods and its characterization |
| topic | T175 Industrial research. Research and development |
| url | http://irep.iium.edu.my/36138/ http://irep.iium.edu.my/36138/ http://irep.iium.edu.my/36138/1/Camera_Ready.pdf http://irep.iium.edu.my/36138/4/1099_Acceptance_%28Included%29.pdf http://irep.iium.edu.my/36138/5/Certificate_of_Participation_%28ID_1099%29.pdf http://irep.iium.edu.my/36138/9/ICBioE2013.pdf |