In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures

© 2017 The Electrochemical Society. Most recently, we developed a phosphotungstic acid impregnated mesoporous silica (PWA-meso-silica) and phosphoric acid doped polybenzimidazole (PA/PBI) composite membrane for use in high temperature fuel cells and achieved exceptional durability under a constant c...

Full description

Bibliographic Details
Main Authors: Zhang, J., Aili, D., Bradley, J., Kuang, H., Pan, C., De Marco, Roland, Li, Q., Jiang, S.
Format: Journal Article
Published: The Electrochemical Society, Inc 2017
Online Access:https://orbit.dtu.dk/en/publications/in-situ-formed-phosphoric-acidphosphosilicate-nanoclusters-in-the
http://hdl.handle.net/20.500.11937/65837
_version_ 1848761215251120128
author Zhang, J.
Aili, D.
Bradley, J.
Kuang, H.
Pan, C.
De Marco, Roland
Li, Q.
Jiang, S.
author_facet Zhang, J.
Aili, D.
Bradley, J.
Kuang, H.
Pan, C.
De Marco, Roland
Li, Q.
Jiang, S.
author_sort Zhang, J.
building Curtin Institutional Repository
collection Online Access
description © 2017 The Electrochemical Society. Most recently, we developed a phosphotungstic acid impregnated mesoporous silica (PWA-meso-silica) and phosphoric acid doped polybenzimidazole (PA/PBI) composite membrane for use in high temperature fuel cells and achieved exceptional durability under a constant current load of 200 mA cm -2 at 200°C for over 2700 h. In this work, the fundamental role of PWA-meso-silica in enhancing the stability of the PA/PBI membrane has been investigated. The microstructure, the PA uptake, swelling ratio, mechanical property and conductivity of PA/PBI/PWA-meso-silica composite membranes depend on the loading of PWA-meso-silica. The results indicate that the optimum limit of PWA-meso-silica loading in the PA/PBI membranes is 15 wt%. Detaled analysis indicates that the mesoporous structure of the PWA-meso-silica framework disintegrates, forming phosphosilicate phases within the PBI polymeric matrix during fuel cell operation at 200°C. The in situ formed phosphosilicates can immobilize a significant amount of PA, forming PA/phosphosilicate nanoclusters that possess high proton conductivity (e.g., 7.2 × 10 -2 S cm -1 at 250°C) and stability and substantially inhibits acid leaching out of themembrane. The substantially reduced acid leaching also alleviates the excess acid in the catalyst layer, reducing the detrimental effect of excess acid on the agglomeration of Pt catalysts especially in the cathode catalyst layer. These phenomena are responsible for the exceptional stability in proton conductivity as well as the significantly reduced agglomeration of Pt nanoparticles in the anode and cathode catalyst layers of PA/PBI/PWA-meso-silica composite membrane fuel cells.
first_indexed 2025-11-14T10:28:08Z
format Journal Article
id curtin-20.500.11937-65837
institution Curtin University Malaysia
institution_category Local University
last_indexed 2025-11-14T10:28:08Z
publishDate 2017
publisher The Electrochemical Society, Inc
recordtype eprints
repository_type Digital Repository
spelling curtin-20.500.11937-658372022-09-01T08:56:57Z In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures Zhang, J. Aili, D. Bradley, J. Kuang, H. Pan, C. De Marco, Roland Li, Q. Jiang, S. © 2017 The Electrochemical Society. Most recently, we developed a phosphotungstic acid impregnated mesoporous silica (PWA-meso-silica) and phosphoric acid doped polybenzimidazole (PA/PBI) composite membrane for use in high temperature fuel cells and achieved exceptional durability under a constant current load of 200 mA cm -2 at 200°C for over 2700 h. In this work, the fundamental role of PWA-meso-silica in enhancing the stability of the PA/PBI membrane has been investigated. The microstructure, the PA uptake, swelling ratio, mechanical property and conductivity of PA/PBI/PWA-meso-silica composite membranes depend on the loading of PWA-meso-silica. The results indicate that the optimum limit of PWA-meso-silica loading in the PA/PBI membranes is 15 wt%. Detaled analysis indicates that the mesoporous structure of the PWA-meso-silica framework disintegrates, forming phosphosilicate phases within the PBI polymeric matrix during fuel cell operation at 200°C. The in situ formed phosphosilicates can immobilize a significant amount of PA, forming PA/phosphosilicate nanoclusters that possess high proton conductivity (e.g., 7.2 × 10 -2 S cm -1 at 250°C) and stability and substantially inhibits acid leaching out of themembrane. The substantially reduced acid leaching also alleviates the excess acid in the catalyst layer, reducing the detrimental effect of excess acid on the agglomeration of Pt catalysts especially in the cathode catalyst layer. These phenomena are responsible for the exceptional stability in proton conductivity as well as the significantly reduced agglomeration of Pt nanoparticles in the anode and cathode catalyst layers of PA/PBI/PWA-meso-silica composite membrane fuel cells. 2017 Journal Article http://hdl.handle.net/20.500.11937/65837 10.1149/2.1051714jes https://orbit.dtu.dk/en/publications/in-situ-formed-phosphoric-acidphosphosilicate-nanoclusters-in-the http://purl.org/au-research/grants/arc/DP150102025 http://purl.org/au-research/grants/arc/DP150102044 The Electrochemical Society, Inc unknown
spellingShingle Zhang, J.
Aili, D.
Bradley, J.
Kuang, H.
Pan, C.
De Marco, Roland
Li, Q.
Jiang, S.
In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures
title In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures
title_full In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures
title_fullStr In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures
title_full_unstemmed In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures
title_short In situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures
title_sort in situ formed phosphoric acid/phosphosilicate nanoclusters in the exceptional enhancement of durability of polybenzimidazole membrane fuel cells at elevated high temperatures
url https://orbit.dtu.dk/en/publications/in-situ-formed-phosphoric-acidphosphosilicate-nanoclusters-in-the
https://orbit.dtu.dk/en/publications/in-situ-formed-phosphoric-acidphosphosilicate-nanoclusters-in-the
https://orbit.dtu.dk/en/publications/in-situ-formed-phosphoric-acidphosphosilicate-nanoclusters-in-the
http://hdl.handle.net/20.500.11937/65837