Workability and compressive strength properties of high strength geopolymer mortars

Geopolymer is an attractive sustainable binder as compared to Ordinary Portland Cement (OPC) in concrete. Recent investigations show that mechanical properties of heat cured geopolymers are similar or comparatively better to those of OPC. However, the requirement of heat curing for fly ash geopolyme...

Full description

Bibliographic Details
Main Authors: Khan, M., Shaikh, Faiz, Hao, Y., Hao, Hong
Format: Conference Paper
Published: 2017
Online Access:http://hdl.handle.net/20.500.11937/60503
_version_ 1848760611440164864
author Khan, M.
Shaikh, Faiz
Hao, Y.
Hao, Hong
author_facet Khan, M.
Shaikh, Faiz
Hao, Y.
Hao, Hong
author_sort Khan, M.
building Curtin Institutional Repository
collection Online Access
description Geopolymer is an attractive sustainable binder as compared to Ordinary Portland Cement (OPC) in concrete. Recent investigations show that mechanical properties of heat cured geopolymers are similar or comparatively better to those of OPC. However, the requirement of heat curing for fly ash geopolymer is not feasible for large scale cast in-situ structural applications. Partial replacement of fly ash with slag has led to the setting of geopolymer mixes at ambient temperature, however the existing combinations in literature realize medium to low compressive strengths at ambient temperature with reduced workability. In this study, high strength ambient cured geopolymer is formed by using low calcium fly ash, Ultra-Fine Fly Ash (UFFA) and ground granulated blast furnace slag (slag). The effect of partial replacement of fly ash with slag (at a higher proportion) and UFFA on the workability of mortar mixtures and the compressive strength gain from 3 to 28 days is presented. Other parameters investigated are the effects of sand/binder ratios and the influence of both air and water curing on the compressive strength development of geopolymer samples. The results suggested that the early age properties of geopolymer can be controlled effectively with the optimum inclusion of additives in low calcium fly ash. Very high compressive strength for geopolymer mixtures up to 110 MPa is achieved at 28 days of ambient air curing. Workability of mixtures decreased with an increase in the additives and sand/binder ratios. Inclusion of superplasticizer (1% by wt. of the binder) slightly improved the workability of mixes having sand/binder of 2.75.
first_indexed 2025-11-14T10:18:32Z
format Conference Paper
id curtin-20.500.11937-60503
institution Curtin University Malaysia
institution_category Local University
last_indexed 2025-11-14T10:18:32Z
publishDate 2017
recordtype eprints
repository_type Digital Repository
spelling curtin-20.500.11937-605032018-08-20T03:23:37Z Workability and compressive strength properties of high strength geopolymer mortars Khan, M. Shaikh, Faiz Hao, Y. Hao, Hong Geopolymer is an attractive sustainable binder as compared to Ordinary Portland Cement (OPC) in concrete. Recent investigations show that mechanical properties of heat cured geopolymers are similar or comparatively better to those of OPC. However, the requirement of heat curing for fly ash geopolymer is not feasible for large scale cast in-situ structural applications. Partial replacement of fly ash with slag has led to the setting of geopolymer mixes at ambient temperature, however the existing combinations in literature realize medium to low compressive strengths at ambient temperature with reduced workability. In this study, high strength ambient cured geopolymer is formed by using low calcium fly ash, Ultra-Fine Fly Ash (UFFA) and ground granulated blast furnace slag (slag). The effect of partial replacement of fly ash with slag (at a higher proportion) and UFFA on the workability of mortar mixtures and the compressive strength gain from 3 to 28 days is presented. Other parameters investigated are the effects of sand/binder ratios and the influence of both air and water curing on the compressive strength development of geopolymer samples. The results suggested that the early age properties of geopolymer can be controlled effectively with the optimum inclusion of additives in low calcium fly ash. Very high compressive strength for geopolymer mixtures up to 110 MPa is achieved at 28 days of ambient air curing. Workability of mixtures decreased with an increase in the additives and sand/binder ratios. Inclusion of superplasticizer (1% by wt. of the binder) slightly improved the workability of mixes having sand/binder of 2.75. 2017 Conference Paper http://hdl.handle.net/20.500.11937/60503 restricted
spellingShingle Khan, M.
Shaikh, Faiz
Hao, Y.
Hao, Hong
Workability and compressive strength properties of high strength geopolymer mortars
title Workability and compressive strength properties of high strength geopolymer mortars
title_full Workability and compressive strength properties of high strength geopolymer mortars
title_fullStr Workability and compressive strength properties of high strength geopolymer mortars
title_full_unstemmed Workability and compressive strength properties of high strength geopolymer mortars
title_short Workability and compressive strength properties of high strength geopolymer mortars
title_sort workability and compressive strength properties of high strength geopolymer mortars
url http://hdl.handle.net/20.500.11937/60503