Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique
The practical use of inorganic hollow fibre membranes has been limited by their brittleness. When assembled inside a membrane module for high temperature applications, the unavoidable thermal expansion or shrinkage would break the membrane. To overcome this problem, in this paper, spiral-shaped poro...
| Main Authors: | , , , , |
|---|---|
| Format: | Journal Article |
| Published: |
Elsevier
2015
|
| Online Access: | http://hdl.handle.net/20.500.11937/6017 |
| _version_ | 1848744957140008960 |
|---|---|
| author | Li, H. Song, J. Tan, X. Jin, Y. Liu, Shaomin |
| author_facet | Li, H. Song, J. Tan, X. Jin, Y. Liu, Shaomin |
| author_sort | Li, H. |
| building | Curtin Institutional Repository |
| collection | Online Access |
| description | The practical use of inorganic hollow fibre membranes has been limited by their brittleness. When assembled inside a membrane module for high temperature applications, the unavoidable thermal expansion or shrinkage would break the membrane. To overcome this problem, in this paper, spiral-shaped porous stainless steel (PSS) hollow fiber membranes have been developed via a modified phase inversion–sintering technique using 316 L stainless steel powder as the membrane material, polysulfone as the polymeric binder and N-methylpyrrolidone as the solvent, respectively. The effects of sintering conditions on the hollow fiber properties have been investigated extensively to optimize the preparation. In order to obtain the desired porous structure, high performance and appropriate mechanical strength, the PSS hollow fiber precursors should be calcined in O2-free sintering atmosphere between 1050 °C and 1100 °C. Under the optimal sintering conditions, the resultant PSS hollow fibre membranes have a bimodal pore size distribution of 0.1–3 μm diameter, high mechanical strength of 290–600 MPa, and the nitrogen permeances ranged between 2.23×10−4 and 2.84×10−5 mol m−2 s−1 Pa−1. When two sides are fixed by sealant, such spiral hollow fiber membranes are able to flexibly expand by 20% and shrink by at most 57% of its original length, thus suitable for variable high-temperature operations as they can offset the thermal expansion and contraction caused by the temperature change. |
| first_indexed | 2025-11-14T06:09:43Z |
| format | Journal Article |
| id | curtin-20.500.11937-6017 |
| institution | Curtin University Malaysia |
| institution_category | Local University |
| last_indexed | 2025-11-14T06:09:43Z |
| publishDate | 2015 |
| publisher | Elsevier |
| recordtype | eprints |
| repository_type | Digital Repository |
| spelling | curtin-20.500.11937-60172017-09-13T14:39:54Z Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique Li, H. Song, J. Tan, X. Jin, Y. Liu, Shaomin The practical use of inorganic hollow fibre membranes has been limited by their brittleness. When assembled inside a membrane module for high temperature applications, the unavoidable thermal expansion or shrinkage would break the membrane. To overcome this problem, in this paper, spiral-shaped porous stainless steel (PSS) hollow fiber membranes have been developed via a modified phase inversion–sintering technique using 316 L stainless steel powder as the membrane material, polysulfone as the polymeric binder and N-methylpyrrolidone as the solvent, respectively. The effects of sintering conditions on the hollow fiber properties have been investigated extensively to optimize the preparation. In order to obtain the desired porous structure, high performance and appropriate mechanical strength, the PSS hollow fiber precursors should be calcined in O2-free sintering atmosphere between 1050 °C and 1100 °C. Under the optimal sintering conditions, the resultant PSS hollow fibre membranes have a bimodal pore size distribution of 0.1–3 μm diameter, high mechanical strength of 290–600 MPa, and the nitrogen permeances ranged between 2.23×10−4 and 2.84×10−5 mol m−2 s−1 Pa−1. When two sides are fixed by sealant, such spiral hollow fiber membranes are able to flexibly expand by 20% and shrink by at most 57% of its original length, thus suitable for variable high-temperature operations as they can offset the thermal expansion and contraction caused by the temperature change. 2015 Journal Article http://hdl.handle.net/20.500.11937/6017 10.1016/j.memsci.2015.04.037 Elsevier restricted |
| spellingShingle | Li, H. Song, J. Tan, X. Jin, Y. Liu, Shaomin Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique |
| title | Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique |
| title_full | Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique |
| title_fullStr | Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique |
| title_full_unstemmed | Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique |
| title_short | Preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique |
| title_sort | preparation of spiral porous stainless steel hollow fiber membranes by a modified phase inversion-sintering technique |
| url | http://hdl.handle.net/20.500.11937/6017 |