Mechanism and Kinetics of SO2 Poisoning on the Electrochemical Activity of La0.8Sr0.2MnO3 Cathodes of Solid Oxide Fuel Cells
The effect of sulfur deposition and poisoning on the electrochemical activity of La0.8Sr0.2MnO3 (LSM) cathode of solid oxide fuel cells (SOFCs) for the O2 reduction reaction is investigated. Sulfur poisoning of the electrochemical activity of LSM electrodes is characterized by two-stage degradation...
| Main Authors: | Wang, Cheng Cheng, Chen, Kongfa, Jiang, San Ping |
|---|---|
| Format: | Journal Article |
| Published: |
The Electrochemical Society, Inc
2016
|
| Online Access: | http://purl.org/au-research/grants/arc/DP150102025 http://hdl.handle.net/20.500.11937/52444 |
Similar Items
Combined Cr and S poisoning of La0.8Sr0.2MnO3-δ (LSM) cathode of solid oxide fuel cells
by: Wang, Cheng Cheng, et al.
Published: (2019)
by: Wang, Cheng Cheng, et al.
Published: (2019)
Chromium deposition and poisoning in dry and humidified air at (La0.8Sr0.2)0.9MnO3+d cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2010)
by: Chen, X., et al.
Published: (2010)
A La0.8Sr0.2MnO3/La0.6Sr0.4Co0.2Fe0.8O3−δ core–shell structured cathode by a rapid sintering process for solid oxide fuel cells
by: Ai, Na, et al.
Published: (2017)
by: Ai, Na, et al.
Published: (2017)
Chromium deposition and poisoning of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Effect of SO2 Poisoning on the Electrochemical Activity of La0.6Sr0.4Co0.2Fe0.8O3-δ Cathodes of Solid Oxide Fuel Cells
by: Wang, C., et al.
Published: (2017)
by: Wang, C., et al.
Published: (2017)
A Fundamental Study of Boron Deposition and Poisoning of La0.8Sr0.2MnO3 Cathode of Solid Oxide Fuel Cells under Accelerated Conditions
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
(La0.8Sr0.2)0.9MnO3–Gd0.2Ce0.8O1.9 composite cathodes prepared from (Gd, Ce)(NO3) x -modified (La0.8Sr0.2)0.9MnO3 for intermediate-temperature solid oxide fuel cells
by: Leng, Y.J., et al.
Published: (2006)
by: Leng, Y.J., et al.
Published: (2006)
A comparative study of La0.8Sr0.2MnO3 and La0.8Sr0.2Sc0.1Mn0.9O3 as cathode materials of single-chamber SOFCs operating on a methane-air mixture
by: Zhang, C., et al.
Published: (2009)
by: Zhang, C., et al.
Published: (2009)
Sulfur Deposition and Poisoning of La0.6Sr0.4Co0.2Fe0.8O3-[delta] Cathode Materials of Solid Oxide Fuel Cells
by: Wang, C., et al.
Published: (2014)
by: Wang, C., et al.
Published: (2014)
A model for the delamination kinetics of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells
by: Zhang, Y., et al.
Published: (2012)
by: Zhang, Y., et al.
Published: (2012)
In situ assembled La0.8Sr0.2MnO3 cathodes on a Y2O3-ZrO2 electrolyte of solid oxide fuel cells-interface and electrochemical activity
by: Li, N., et al.
Published: (2016)
by: Li, N., et al.
Published: (2016)
Performance and stability of La0.8Sr0.2MnO3 cathode promoted with palladium based catalysts in solid oxide fuel cells
by: Babaei, A., et al.
Published: (2011)
by: Babaei, A., et al.
Published: (2011)
Performance and structural stability of Gd0.2Ce0.8O1.9 infiltrated La0.8Sr0.2MnO3 nanostructured oxygen electrodes of solid oxide electrolysis cells
by: Chen, Kongfa, et al.
Published: (2014)
by: Chen, Kongfa, et al.
Published: (2014)
Boron deposition and poisoning of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells under accelerated operation conditions
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Effect of temperature on the chromium deposition and poisoning of La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes of solid oxide fuel cells
by: Wang, C., et al.
Published: (2014)
by: Wang, C., et al.
Published: (2014)
A fundamental study of chromium depostion and poisoning at (La0.8Sr0.2)0.95(Mn1-xCox)O3 cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2011)
by: Chen, X., et al.
Published: (2011)
A new symmetric solid-oxide fuel cell with La0.8Sr0.2Sc0.2Mn0.8O3-d perovskite oxide as both the anode and cathode
by: Zheng, Y., et al.
Published: (2009)
by: Zheng, Y., et al.
Published: (2009)
Activation and deactivation kinetics of oxygen reduction over a la 0.8Sr0.2Sc0.1Mn0.9O3 cathode
by: Zheng, Y., et al.
Published: (2008)
by: Zheng, Y., et al.
Published: (2008)
Chromium deposition and poisoning at La0.6Sr0.4Co0.2Fe0.8O3d oxygen electrodes of solid oxide electrolysis cells
by: Wei, B., et al.
Published: (2015)
by: Wei, B., et al.
Published: (2015)
Surface segregation and chromium deposition and poisoning on La 0.6Sr0.4Co0.2Fe0.8O 3-d cathodes of solid oxide fuel cells
by: Zhao, L., et al.
Published: (2013)
by: Zhao, L., et al.
Published: (2013)
Chromium deposition and poisoning on (La0.6 Sr0.4-x Bax) (Co0.2 Fe0.8) O3 (0=x= 0.4) cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2008)
by: Chen, X., et al.
Published: (2008)
Synergistic effects of temperature and polarization on Cr poisoning of La0.6Sr0.4Co0.2Fe0.8O3-: δ solid oxide fuel cell cathodes
by: Ni, N., et al.
Published: (2019)
by: Ni, N., et al.
Published: (2019)
Study on oxygen activation and methane oxidation over La0.8Sr0.2MnO3 electrode in single-chamber solid oxide fuel cells via an electrochemical approach
by: Zheng, Y., et al.
Published: (2012)
by: Zheng, Y., et al.
Published: (2012)
Electrical and magneto-transport properties of magneto-resistive la0.7Ca0.28Sr0.2 MnO3 prepared at different sintering temperature
by: Ewe, L.S, et al.
Published: (2012)
by: Ewe, L.S, et al.
Published: (2012)
Chromium deposition and poisoning at Ba0.5Sr0.5Co0.8Fe0.2O3 cathode of solid oxide fuel cells
by: Kim, Y., et al.
Published: (2011)
by: Kim, Y., et al.
Published: (2011)
Study of structure, microstructure and electrical properties of La0.8Na0.2MnO3 in bulk and thin film
by: Ng, Siau Wei, et al.
Published: (2010)
by: Ng, Siau Wei, et al.
Published: (2010)
Magnetotransport and electrical properties of colossal magnetoresistive La0.8Sr0.2Mn03 at different sintering temperature.
by: Lim, Kean Pah, et al.
Published: (2011)
by: Lim, Kean Pah, et al.
Published: (2011)
Interface formation and Mn segregation of directly assembled La0.8Sr0.2MnO3 cathode on Y2O3-ZrO2 and Gd2O3-CeO2 electrolytes of solid oxide fuel cells
by: He, S., et al.
Published: (2018)
by: He, S., et al.
Published: (2018)
Highly chromium contaminant tolerant BaO infiltrated La0.6Sr0.4Co0.2Fe0.8O3-delta cathodes for solid oxide fuel cells
by: Chen, Kongfa, et al.
Published: (2015)
by: Chen, Kongfa, et al.
Published: (2015)
Thermodynamic stability mapping and electrochemical study of La1-xSrxCo0.2Fe0.8O3±δ (x=0.2–0.4) as a cathode of solid oxide fuel cells in the presence of SO2
by: Darvish, S., et al.
Published: (2018)
by: Darvish, S., et al.
Published: (2018)
Assessment of nickel cermets and La0.8Sr0.2Sc0.2Mn0.8O3 as solid-oxide fuel cell anodes operating on carbon monoxide fuel
by: Su, C., et al.
Published: (2010)
by: Su, C., et al.
Published: (2010)
Electrochemical performance of SrSc0.2Co0.8O 3-d cathode on Sm0.2Ce0.8O1.9 electrolyte for low temperature SOFCs
by: Zhou, W., et al.
Published: (2009)
by: Zhou, W., et al.
Published: (2009)
Highly sulfur poisoning-tolerant BaCeO3-impregnated La0.6Sr0.4Co0.2Fe0.8O3−δ cathodes for solid oxide fuel cells
by: Wang, C., et al.
Published: (2018)
by: Wang, C., et al.
Published: (2018)
Performance stability and degradation mechanism of La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes under solid oxide fuel cells operation conditions
by: Liu, Y., et al.
Published: (2014)
by: Liu, Y., et al.
Published: (2014)
A FIB-STEM study of La0.8Sr0.2MnO3 Cathode and Y2O3-ZrO2/Gd2O3-CeO2 electrolyte interfaces of solid oxide fuel cells
by: He, Shuai, et al.
Published: (2017)
by: He, Shuai, et al.
Published: (2017)
Enhanced Chromium Tolerance of La0.6Sr0.4Co0.2Fe0.8O3-δ Cathode by BaO Infiltration
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Colossal Magnetoresistance of (La1-xDyx)0.67Sr0.33MnO3 Perovskite
by: Lim, Kean Pah, et al.
Published: (2007)
by: Lim, Kean Pah, et al.
Published: (2007)
Structural, microstructural and electrical properties of La0.67(Ba,Sr)0.33MnO3 system
by: Gan, Albert Han Ming, et al.
Published: (2010)
by: Gan, Albert Han Ming, et al.
Published: (2010)
The physical properties of submicron and nano-grained La0.7Sr0.3MnO3 and Nd0.7Sr0.3MnO3 synthesised by sol–gel and solid-state reaction methods
by: Lau, Lik Nguong, et al.
Published: (2021)
by: Lau, Lik Nguong, et al.
Published: (2021)
Palladium and ceria infiltrated La0.8Sr0.2Co0.5Fe0.5O3-[delta] cathodes of solid oxide fuel cells
by: Chen, J., et al.
Published: (2009)
by: Chen, J., et al.
Published: (2009)
Similar Items
-
Combined Cr and S poisoning of La0.8Sr0.2MnO3-δ (LSM) cathode of solid oxide fuel cells
by: Wang, Cheng Cheng, et al.
Published: (2019) -
Chromium deposition and poisoning in dry and humidified air at (La0.8Sr0.2)0.9MnO3+d cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2010) -
A La0.8Sr0.2MnO3/La0.6Sr0.4Co0.2Fe0.8O3−δ core–shell structured cathode by a rapid sintering process for solid oxide fuel cells
by: Ai, Na, et al.
Published: (2017) -
Chromium deposition and poisoning of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells
by: Chen, K., et al.
Published: (2015) -
Effect of SO2 Poisoning on the Electrochemical Activity of La0.6Sr0.4Co0.2Fe0.8O3-δ Cathodes of Solid Oxide Fuel Cells
by: Wang, C., et al.
Published: (2017)