Surface segregation and chromium deposition and poisoning on La 0.6Sr0.4Co0.2Fe0.8O 3-d cathodes of solid oxide fuel cells
La0.6Sr0.4Co0.2Fe0.8O 3-d, (LSCF) perovskite oxide is one of the most common cathode materials used in solid oxide fuel cells (IT-SOFCs), but vulnerable to the chromium deposition and poisoning in the presence of gaseous chromium species from metallic interconnect. In this work, the fundamental rela...
| Main Authors: | Zhao, L., Drennan, J., Kong, C., Amarasinghe, S., Jiang, San Ping |
|---|---|
| Format: | Journal Article |
| Published: |
Electrochemical Society Inc.
2013
|
| Online Access: | http://hdl.handle.net/20.500.11937/34922 |
Similar Items
Insight into surface segregation and chromium deposition on La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes of solid oxide fuel cells
by: Zhao, L., et al.
Published: (2014)
by: Zhao, L., et al.
Published: (2014)
Chromium deposition and poisoning on (La0.6 Sr0.4-x Bax) (Co0.2 Fe0.8) O3 (0=x= 0.4) cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2008)
by: Chen, X., et al.
Published: (2008)
Effect of temperature on the chromium deposition and poisoning of La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes of solid oxide fuel cells
by: Wang, C., et al.
Published: (2014)
by: Wang, C., et al.
Published: (2014)
Enhanced Chromium Tolerance of La0.6Sr0.4Co0.2Fe0.8O3-δ Cathode by BaO Infiltration
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Sulfur Deposition and Poisoning of La0.6Sr0.4Co0.2Fe0.8O3-[delta] Cathode Materials of Solid Oxide Fuel Cells
by: Wang, C., et al.
Published: (2014)
by: Wang, C., et al.
Published: (2014)
Chromium and Sulfur Contaminants on La0.6Sr0.4Co0.2Fe0.8O3-δ Cathodes of Solid Oxide Fuel Cells
by: Wang, C., et al.
Published: (2015)
by: Wang, C., et al.
Published: (2015)
Chromium deposition and poisoning at La0.6Sr0.4Co0.2Fe0.8O3d oxygen electrodes of solid oxide electrolysis cells
by: Wei, B., et al.
Published: (2015)
by: Wei, B., et al.
Published: (2015)
Chromium deposition and poisoning at Ba0.5Sr0.5Co0.8Fe0.2O3 cathode of solid oxide fuel cells
by: Kim, Y., et al.
Published: (2011)
by: Kim, Y., et al.
Published: (2011)
Enhanced chromium tolerance of Gd0.1Ce0.9O 1.95 Impregnated La0.6Sr0.4Co 0.2Fe0.8O3-d electrode of solid oxide fuel cells
by: Zhao, L., et al.
Published: (2013)
by: Zhao, L., et al.
Published: (2013)
Enhanced chromium tolerance of La0.6Sr0.4Co0.2Fe0.8O3 − δ electrode of solid oxide fuel cells by Gd0.1Ce0.9O1.95 impregnation
by: Zhao, L., et al.
Published: (2013)
by: Zhao, L., et al.
Published: (2013)
Chromium deposition and poisoning in dry and humidified air at (La0.8Sr0.2)0.9MnO3+d cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2010)
by: Chen, X., et al.
Published: (2010)
Raman Spectroscopy Study of Chromium Deposition on La0.6Sr0.4Co0.2Fe0.8O3-δ Cathode of Solid Oxide Fuel Cells
by: Zhao, L., et al.
Published: (2014)
by: Zhao, L., et al.
Published: (2014)
Synergistic effects of temperature and polarization on Cr poisoning of La0.6Sr0.4Co0.2Fe0.8O3-: δ solid oxide fuel cell cathodes
by: Ni, N., et al.
Published: (2019)
by: Ni, N., et al.
Published: (2019)
Effect of SO2 Poisoning on the Electrochemical Activity of La0.6Sr0.4Co0.2Fe0.8O3-δ Cathodes of Solid Oxide Fuel Cells
by: Wang, C., et al.
Published: (2017)
by: Wang, C., et al.
Published: (2017)
A fundamental study of chromium depostion and poisoning at (La0.8Sr0.2)0.95(Mn1-xCox)O3 cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2011)
by: Chen, X., et al.
Published: (2011)
A La0.8Sr0.2MnO3/La0.6Sr0.4Co0.2Fe0.8O3−δ core–shell structured cathode by a rapid sintering process for solid oxide fuel cells
by: Ai, Na, et al.
Published: (2017)
by: Ai, Na, et al.
Published: (2017)
Highly sulfur poisoning-tolerant BaCeO3-impregnated La0.6Sr0.4Co0.2Fe0.8O3−δ cathodes for solid oxide fuel cells
by: Wang, C., et al.
Published: (2018)
by: Wang, C., et al.
Published: (2018)
Chromium deposition and poisoning of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Highly chromium contaminant tolerant BaO infiltrated La0.6Sr0.4Co0.2Fe0.8O3-delta cathodes for solid oxide fuel cells
by: Chen, Kongfa, et al.
Published: (2015)
by: Chen, Kongfa, et al.
Published: (2015)
Combined Cr and S poisoning of La0.8Sr0.2MnO3-δ (LSM) cathode of solid oxide fuel cells
by: Wang, Cheng Cheng, et al.
Published: (2019)
by: Wang, Cheng Cheng, et al.
Published: (2019)
Mechanism and Kinetics of SO2 Poisoning on the Electrochemical Activity of La0.8Sr0.2MnO3 Cathodes of Solid Oxide Fuel Cells
by: Wang, Cheng Cheng, et al.
Published: (2016)
by: Wang, Cheng Cheng, et al.
Published: (2016)
(La0.8Sr0.2)0.9MnO3–Gd0.2Ce0.8O1.9 composite cathodes prepared from (Gd, Ce)(NO3) x -modified (La0.8Sr0.2)0.9MnO3 for intermediate-temperature solid oxide fuel cells
by: Leng, Y.J., et al.
Published: (2006)
by: Leng, Y.J., et al.
Published: (2006)
Performance stability and degradation mechanism of La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes under solid oxide fuel cells operation conditions
by: Liu, Y., et al.
Published: (2014)
by: Liu, Y., et al.
Published: (2014)
Palladium and ceria infiltrated La0.8Sr0.2Co0.5Fe0.5O3-[delta] cathodes of solid oxide fuel cells
by: Chen, J., et al.
Published: (2009)
by: Chen, J., et al.
Published: (2009)
Study on the Cr deposition and poisoning phenomenon at (La0.6Sr0.4)(Co0.2Fe0.8)O3-d electrode of solid oxide fuel cells by transmission X-ray microscopy
by: Chen, X., et al.
Published: (2014)
by: Chen, X., et al.
Published: (2014)
Evaluation of La0.6Sr0.4Co0.2Fe0.8O3-δ as a potential cathode for proton-conducting solid oxide fuel cell
by: Ismariza Ismail,, et al.
Published: (2018)
by: Ismariza Ismail,, et al.
Published: (2018)
Effect of strontium content on chromium deposition and poisoning in Ba1-xSrxCo0.8Fe0.2O3-δ (0.3≤ x ≤0.7) cathodes of solid oxide fuel cells
by: Kim, Y., et al.
Published: (2012)
by: Kim, Y., et al.
Published: (2012)
A Fundamental Study of Boron Deposition and Poisoning of La0.8Sr0.2MnO3 Cathode of Solid Oxide Fuel Cells under Accelerated Conditions
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
A comparative study of La0.8Sr0.2MnO3 and La0.8Sr0.2Sc0.1Mn0.9O3 as cathode materials of single-chamber SOFCs operating on a methane-air mixture
by: Zhang, C., et al.
Published: (2009)
by: Zhang, C., et al.
Published: (2009)
Suppressed Sr segregation and performance of directly assembled La0.6Sr0.4Co0.2Fe0.8O3-δ oxygen electrode on Y2O3-ZrO2 electrolyte of solid oxide electrolysis cells
by: Ai, N., et al.
Published: (2018)
by: Ai, N., et al.
Published: (2018)
Cr deposition on porous La0.6Sr0.4Co0.2Fe0.8O3 − δ electrodes of solid oxide cells under open circuit condition
by: Wei, B., et al.
Published: (2015)
by: Wei, B., et al.
Published: (2015)
Influence of nitric oxide on the oxygen permeation behavior of La0.6Sr0.4Co0.2Fe0.8O3-?perovskite membranes
by: Gao, J., et al.
Published: (2019)
by: Gao, J., et al.
Published: (2019)
Palladium surface modified La(0.6)Sr(0.4)Co(0.2)Fe(0.8)O(3-δ) hollow fibres for oxygen separation
by: Yacou, C., et al.
Published: (2011)
by: Yacou, C., et al.
Published: (2011)
A FIB-STEM Study of Strontium Segregation and Interface Formation of Directly Assembled La0.6Sr0.4Co0.2Fe0.8O3.delta Cathode on Y2O3-ZrO2 Electrolyte of Solid Oxide Fuel Cells
by: He, Shuai, et al.
Published: (2018)
by: He, Shuai, et al.
Published: (2018)
Properties and performance of Ba0.5Sr0.5Co0.8Fe0.2O3-d + Sm0.2Ce0.8O1.9 composite cathode
by: Wang, K., et al.
Published: (2008)
by: Wang, K., et al.
Published: (2008)
Polarization-Induced Interface and Sr Segregation of in Situ Assembled La0.6Sr0.4Co0.2Fe0.8O3−δ Electrodes on Y2O3–ZrO2 Electrolyte of Solid Oxide Fuel Cells
by: Chen, K., et al.
Published: (2016)
by: Chen, K., et al.
Published: (2016)
Activation and deactivation kinetics of oxygen reduction over a la 0.8Sr0.2Sc0.1Mn0.9O3 cathode
by: Zheng, Y., et al.
Published: (2008)
by: Zheng, Y., et al.
Published: (2008)
Electrochemical performance of La0.6Sr0.4Co0.2Fe0.8O3-δ cathode material prepared by a sol-gel method assisted with functionalized carbon nanotubes
by: Nurul Izzati Abd Malek,, et al.
Published: (2020)
by: Nurul Izzati Abd Malek,, et al.
Published: (2020)
Sintering and oxygen permeation studies of La0.6Sr0.4Co0.2Fe0.8O3-δ ceramic membranes with improved purity
by: Zou, Y., et al.
Published: (2011)
by: Zou, Y., et al.
Published: (2011)
Significant effects of sintering temperature on the performance of La0.6Sr0.4Co0.2Fe0.8O3-d oxygen selective membranes
by: Zeng, P., et al.
Published: (2007)
by: Zeng, P., et al.
Published: (2007)
Similar Items
-
Insight into surface segregation and chromium deposition on La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes of solid oxide fuel cells
by: Zhao, L., et al.
Published: (2014) -
Chromium deposition and poisoning on (La0.6 Sr0.4-x Bax) (Co0.2 Fe0.8) O3 (0=x= 0.4) cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2008) -
Effect of temperature on the chromium deposition and poisoning of La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes of solid oxide fuel cells
by: Wang, C., et al.
Published: (2014) -
Enhanced Chromium Tolerance of La0.6Sr0.4Co0.2Fe0.8O3-δ Cathode by BaO Infiltration
by: Chen, K., et al.
Published: (2015) -
Sulfur Deposition and Poisoning of La0.6Sr0.4Co0.2Fe0.8O3-[delta] Cathode Materials of Solid Oxide Fuel Cells
by: Wang, C., et al.
Published: (2014)