Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures

The loaded salts (NaCl, KCl, MgCl2, and CaCl2) have significantly different influence on the contribution of dehydration and depolymerization reactions to the decomposition of sugar structures during cellulose fast pyrolysis at 325 C. The structures of salt-loaded celluloses already become cross-lin...

Full description

Bibliographic Details
Main Authors: Liu, Dawei, Yu, Yun, Hayashi, J., Moghtaderi, B., Wu, Hongwei
Format: Journal Article
Published: Elsevier Ltd 2014
Online Access:http://hdl.handle.net/20.500.11937/3383
_version_ 1848744216437456896
author Liu, Dawei
Yu, Yun
Hayashi, J.
Moghtaderi, B.
Wu, Hongwei
author_facet Liu, Dawei
Yu, Yun
Hayashi, J.
Moghtaderi, B.
Wu, Hongwei
author_sort Liu, Dawei
building Curtin Institutional Repository
collection Online Access
description The loaded salts (NaCl, KCl, MgCl2, and CaCl2) have significantly different influence on the contribution of dehydration and depolymerization reactions to the decomposition of sugar structures during cellulose fast pyrolysis at 325 C. The structures of salt-loaded celluloses already become cross-linked during heating-up period, largely due to the enhanced dehydration reactions catalyzed by inorganic species. As stronger Lewis acids, the alkaline earth metal ions (Mg2+ and Ca2+) are more effective than the alkali metal ions (Na+ and K+) to catalyze the dehydration reactions of sugar structures, leading to the formation of more cross-linked cellulose for the alkaline earth metal chloride-loaded celluloses. As a result, the majority of Mg and Ca are transformed into water-insoluble forms during the heating-up period, largely reducing the catalytic effects of these species on the dehydration of sugar structures during the subsequent isothermal pyrolysis. Rather, the dehydration of non-sugar structures is enhanced because the catalytic species are already bonded with non-sugar structures. In contrast, the dehydration of sugar structures during the heating-up period is less significant for the NaCl-loaded and KCl-loaded celluloses.The majority of Na and K are water-soluble after the heating-up period so that the dehydration of sugar structures is further enhanced during isothermal pyrolysis. The loaded salts have less influence on the depolymerization reactions. The contribution of depolymerization reactions to sugar conversion is relatively small during the heating-up stage, but increases substantially during isothermal pyrolysis.
first_indexed 2025-11-14T05:57:56Z
format Journal Article
id curtin-20.500.11937-3383
institution Curtin University Malaysia
institution_category Local University
last_indexed 2025-11-14T05:57:56Z
publishDate 2014
publisher Elsevier Ltd
recordtype eprints
repository_type Digital Repository
spelling curtin-20.500.11937-33832017-09-13T16:01:58Z Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures Liu, Dawei Yu, Yun Hayashi, J. Moghtaderi, B. Wu, Hongwei The loaded salts (NaCl, KCl, MgCl2, and CaCl2) have significantly different influence on the contribution of dehydration and depolymerization reactions to the decomposition of sugar structures during cellulose fast pyrolysis at 325 C. The structures of salt-loaded celluloses already become cross-linked during heating-up period, largely due to the enhanced dehydration reactions catalyzed by inorganic species. As stronger Lewis acids, the alkaline earth metal ions (Mg2+ and Ca2+) are more effective than the alkali metal ions (Na+ and K+) to catalyze the dehydration reactions of sugar structures, leading to the formation of more cross-linked cellulose for the alkaline earth metal chloride-loaded celluloses. As a result, the majority of Mg and Ca are transformed into water-insoluble forms during the heating-up period, largely reducing the catalytic effects of these species on the dehydration of sugar structures during the subsequent isothermal pyrolysis. Rather, the dehydration of non-sugar structures is enhanced because the catalytic species are already bonded with non-sugar structures. In contrast, the dehydration of sugar structures during the heating-up period is less significant for the NaCl-loaded and KCl-loaded celluloses.The majority of Na and K are water-soluble after the heating-up period so that the dehydration of sugar structures is further enhanced during isothermal pyrolysis. The loaded salts have less influence on the depolymerization reactions. The contribution of depolymerization reactions to sugar conversion is relatively small during the heating-up stage, but increases substantially during isothermal pyrolysis. 2014 Journal Article http://hdl.handle.net/20.500.11937/3383 10.1016/j.fuel.2014.07.025 Elsevier Ltd restricted
spellingShingle Liu, Dawei
Yu, Yun
Hayashi, J.
Moghtaderi, B.
Wu, Hongwei
Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures
title Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures
title_full Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures
title_fullStr Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures
title_full_unstemmed Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures
title_short Contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures
title_sort contribution of dehydration and depolymerization reactions during the fast pyrolysis of various salt-loaded celluloses at low temperatures
url http://hdl.handle.net/20.500.11937/3383