Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO

A series of ZnO photocatalysts doped with different amounts of cerium were prepared by co-precipitation and then calcined at different temperatures. The prepared pure ZnO and Ce-doped ZnO samples were characterized by X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, scanning...

Full description

Bibliographic Details
Main Authors: Yu, C., Yang, K., Yu, J., Peng, P., Cao, F., Li, Xin Yong, Zhou, X.
Format: Journal Article
Published: 2011
Online Access:http://hdl.handle.net/20.500.11937/30898
_version_ 1848753222742704128
author Yu, C.
Yang, K.
Yu, J.
Peng, P.
Cao, F.
Li, Xin Yong
Zhou, X.
author_facet Yu, C.
Yang, K.
Yu, J.
Peng, P.
Cao, F.
Li, Xin Yong
Zhou, X.
author_sort Yu, C.
building Curtin Institutional Repository
collection Online Access
description A series of ZnO photocatalysts doped with different amounts of cerium were prepared by co-precipitation and then calcined at different temperatures. The prepared pure ZnO and Ce-doped ZnO samples were characterized by X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, scanning electron microscopy (SEM), UV-visible (UV-Vis) spectroscopy, and photoluminescence (PL) spectroscopy. The photocatalytic activity of the samples was evaluated by the photodegradation of acid orange II under UV light (?=365 nm) irradiation. FT-IR results showed that ZnO doped with 2% (w, mass fraction) cerium had far more OH groups over the surface of the doped sample than the pure ZnO. At the same time, PL tests indicated that the presence of 2% (w) cerium effectively suppressed the recombination of the photogenerated hole-electron pairs. On the other hand, the calcination temperatures influenced the crystallinity and crystal size of the catalysts. XRD tests indicated that the sample calcined at 500 °C had good crystallinity and a small crystal size while elevated temperature treatment (600-800 °C) would result in sintering and increase the crystal size. At the optimal calcination temperature of 500 °C and at 2% (w) cerium doping the composite photocatalyst had much higher photocatalytic activity and stability compared with pure ZnO. The high photocatalytic performance of the Ce doped ZnO could be attributed to an increase in surface OH groups, high crystallinity and a low recombination rate of electron/hole (e-/h+) pairs. © Editorial office of Acta Physico-Chimica Sinica.
first_indexed 2025-11-14T08:21:05Z
format Journal Article
id curtin-20.500.11937-30898
institution Curtin University Malaysia
institution_category Local University
last_indexed 2025-11-14T08:21:05Z
publishDate 2011
recordtype eprints
repository_type Digital Repository
spelling curtin-20.500.11937-308982017-01-30T13:22:11Z Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO Yu, C. Yang, K. Yu, J. Peng, P. Cao, F. Li, Xin Yong Zhou, X. A series of ZnO photocatalysts doped with different amounts of cerium were prepared by co-precipitation and then calcined at different temperatures. The prepared pure ZnO and Ce-doped ZnO samples were characterized by X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, scanning electron microscopy (SEM), UV-visible (UV-Vis) spectroscopy, and photoluminescence (PL) spectroscopy. The photocatalytic activity of the samples was evaluated by the photodegradation of acid orange II under UV light (?=365 nm) irradiation. FT-IR results showed that ZnO doped with 2% (w, mass fraction) cerium had far more OH groups over the surface of the doped sample than the pure ZnO. At the same time, PL tests indicated that the presence of 2% (w) cerium effectively suppressed the recombination of the photogenerated hole-electron pairs. On the other hand, the calcination temperatures influenced the crystallinity and crystal size of the catalysts. XRD tests indicated that the sample calcined at 500 °C had good crystallinity and a small crystal size while elevated temperature treatment (600-800 °C) would result in sintering and increase the crystal size. At the optimal calcination temperature of 500 °C and at 2% (w) cerium doping the composite photocatalyst had much higher photocatalytic activity and stability compared with pure ZnO. The high photocatalytic performance of the Ce doped ZnO could be attributed to an increase in surface OH groups, high crystallinity and a low recombination rate of electron/hole (e-/h+) pairs. © Editorial office of Acta Physico-Chimica Sinica. 2011 Journal Article http://hdl.handle.net/20.500.11937/30898 restricted
spellingShingle Yu, C.
Yang, K.
Yu, J.
Peng, P.
Cao, F.
Li, Xin Yong
Zhou, X.
Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO
title Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO
title_full Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO
title_fullStr Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO
title_full_unstemmed Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO
title_short Effects of rare earth Ce doping on the structure and photocatalytic performance of ZnO
title_sort effects of rare earth ce doping on the structure and photocatalytic performance of zno
url http://hdl.handle.net/20.500.11937/30898