(La0.8Sr0.2)0.9MnO3–Gd0.2Ce0.8O1.9 composite cathodes prepared from (Gd, Ce)(NO3) x -modified (La0.8Sr0.2)0.9MnO3 for intermediate-temperature solid oxide fuel cells
| Main Authors: | Leng, Y.J., Chan, S.H., Khor, K.A., Jiang, San Ping |
|---|---|
| Format: | Journal Article |
| Published: |
Springer
2006
|
| Online Access: | http://www.springerlink.com/content/vj3343219k527878/fulltext.html http://hdl.handle.net/20.500.11937/23313 |
Similar Items
Performance and structural stability of Gd0.2Ce0.8O1.9 infiltrated La0.8Sr0.2MnO3 nanostructured oxygen electrodes of solid oxide electrolysis cells
by: Chen, Kongfa, et al.
Published: (2014)
by: Chen, Kongfa, et al.
Published: (2014)
A comparative study of La0.8Sr0.2MnO3 and La0.8Sr0.2Sc0.1Mn0.9O3 as cathode materials of single-chamber SOFCs operating on a methane-air mixture
by: Zhang, C., et al.
Published: (2009)
by: Zhang, C., et al.
Published: (2009)
Ce0.9Gd0.1O2−δ membranes coated with porous Ba0.5Sr0.5Co0.8Fe0.2O3−δ for oxygen separation
by: Zhang, C., et al.
Published: (2015)
by: Zhang, C., et al.
Published: (2015)
Chromium deposition and poisoning in dry and humidified air at (La0.8Sr0.2)0.9MnO3+d cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2010)
by: Chen, X., et al.
Published: (2010)
Properties and performance of Ba0.5Sr0.5Co0.8Fe0.2O3-d + Sm0.2Ce0.8O1.9 composite cathode
by: Wang, K., et al.
Published: (2008)
by: Wang, K., et al.
Published: (2008)
Activation and deactivation kinetics of oxygen reduction over a la 0.8Sr0.2Sc0.1Mn0.9O3 cathode
by: Zheng, Y., et al.
Published: (2008)
by: Zheng, Y., et al.
Published: (2008)
Electrochemical performance of SrSc0.2Co0.8O 3-d cathode on Sm0.2Ce0.8O1.9 electrolyte for low temperature SOFCs
by: Zhou, W., et al.
Published: (2009)
by: Zhou, W., et al.
Published: (2009)
Enhanced chromium tolerance of Gd0.1Ce0.9O 1.95 Impregnated La0.6Sr0.4Co 0.2Fe0.8O3-d electrode of solid oxide fuel cells
by: Zhao, L., et al.
Published: (2013)
by: Zhao, L., et al.
Published: (2013)
Enhanced chromium tolerance of La0.6Sr0.4Co0.2Fe0.8O3 − δ electrode of solid oxide fuel cells by Gd0.1Ce0.9O1.95 impregnation
by: Zhao, L., et al.
Published: (2013)
by: Zhao, L., et al.
Published: (2013)
A La0.8Sr0.2MnO3/La0.6Sr0.4Co0.2Fe0.8O3−δ core–shell structured cathode by a rapid sintering process for solid oxide fuel cells
by: Ai, Na, et al.
Published: (2017)
by: Ai, Na, et al.
Published: (2017)
Electrochemical Performance of Ba0.5Sr0.5Co0.8Fe0.2O3−δ in Symmetric Cells With Sm0.2Ce0.8O1.9 Electrolyte for Nitric Oxide Reduction Reaction
by: Shi, Huangang, et al.
Published: (2020)
by: Shi, Huangang, et al.
Published: (2020)
Ba and Gd Doping Effect in (BaxSr1–x)0.95Gd0.05Co0.8Fe0.2O3–d (x = 0.1–0.9) Cathode on the Phase Structure and Electrochemical Performance
by: Li, Z., et al.
Published: (2012)
by: Li, Z., et al.
Published: (2012)
Chromium deposition and poisoning of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Assessment of nickel cermets and La0.8Sr0.2Sc0.2Mn0.8O3 as solid-oxide fuel cell anodes operating on carbon monoxide fuel
by: Su, C., et al.
Published: (2010)
by: Su, C., et al.
Published: (2010)
A composite oxygen-reduction electrode composed of SrSc 0.2Co0.8O3-d perovskite and Sm 0.2Ce0.8O1.9 for an intermediate-temperature solid-oxide fuel cell
by: An, B., et al.
Published: (2010)
by: An, B., et al.
Published: (2010)
Combined Cr and S poisoning of La0.8Sr0.2MnO3-δ (LSM) cathode of solid oxide fuel cells
by: Wang, Cheng Cheng, et al.
Published: (2019)
by: Wang, Cheng Cheng, et al.
Published: (2019)
A model for the delamination kinetics of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells
by: Zhang, Y., et al.
Published: (2012)
by: Zhang, Y., et al.
Published: (2012)
Enhanced Oxygen Permeation Behavior of Ba0.5Sr0.5Co0.8Fe0.2O3-d Membranes in a CO2-Containing Atmosphere with a Sm0.2Ce0.8O1.9 Functional Shell
by: Zhang, K., et al.
Published: (2016)
by: Zhang, K., et al.
Published: (2016)
A new symmetric solid-oxide fuel cell with La0.8Sr0.2Sc0.2Mn0.8O3-d perovskite oxide as both the anode and cathode
by: Zheng, Y., et al.
Published: (2009)
by: Zheng, Y., et al.
Published: (2009)
Effect of heat treatment on the structural, morphology and electrochemical performance of perovskite Ba0.5Sr0.5Co0.8Fe0.2O3−δ-Sm0.2Ce0.8O1.9 carbonate protective coating for SOFC metallic interconnect
by: Tan, Kang Huai, et al.
Published: (2020)
by: Tan, Kang Huai, et al.
Published: (2020)
Performance and stability of La0.8Sr0.2MnO3 cathode promoted with palladium based catalysts in solid oxide fuel cells
by: Babaei, A., et al.
Published: (2011)
by: Babaei, A., et al.
Published: (2011)
Composite fuel electrode La0.2Sr0.8TiO3–σ-Ce0.8Sm0.2O2-σ for electrolysis of CO2 in an oxygen-ion conducting solid oxide electrolyser
by: Li, Y., et al.
Published: (2012)
by: Li, Y., et al.
Published: (2012)
Study of structure, microstructure and electrical properties of La0.8Na0.2MnO3 in bulk and thin film
by: Ng, Siau Wei, et al.
Published: (2010)
by: Ng, Siau Wei, et al.
Published: (2010)
Oxygen permeation behavior through Ce0.9Gd0.1O2−δ membranes electronically short-circuited by dual-phase Ce0.9Gd0.1O2−δ–Ag decoration
by: Zhang, C., et al.
Published: (2015)
by: Zhang, C., et al.
Published: (2015)
Interface formation and Mn segregation of directly assembled La0.8Sr0.2MnO3 cathode on Y2O3-ZrO2 and Gd2O3-CeO2 electrolytes of solid oxide fuel cells
by: He, S., et al.
Published: (2018)
by: He, S., et al.
Published: (2018)
Mechanism and Kinetics of SO2 Poisoning on the Electrochemical Activity of La0.8Sr0.2MnO3 Cathodes of Solid Oxide Fuel Cells
by: Wang, Cheng Cheng, et al.
Published: (2016)
by: Wang, Cheng Cheng, et al.
Published: (2016)
La0.6Sr0.4Co0.2Fe0.8O3-d Hollow Fibre Membrane Performance Improvement by Coating of Ba0.5Sr0.5Co0.9Nb0.1O3-d Porous Layer
by: Han, D., et al.
Published: (2014)
by: Han, D., et al.
Published: (2014)
A FIB-STEM study of La0.8Sr0.2MnO3 Cathode and Y2O3-ZrO2/Gd2O3-CeO2 electrolyte interfaces of solid oxide fuel cells
by: He, Shuai, et al.
Published: (2017)
by: He, Shuai, et al.
Published: (2017)
Enhanced oxygen permeability and electronic conductivity of Ce0.8Gd0.2O2 − δ membrane via the addition of sintering aids
by: Zhang, C., et al.
Published: (2017)
by: Zhang, C., et al.
Published: (2017)
Boron deposition and poisoning of La0.8Sr0.2MnO3 oxygen electrodes of solid oxide electrolysis cells under accelerated operation conditions
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Zirconium doping effect on the performance of proton-conducting BaZryCe0.8-yY0.2O3-d (0.0 = y = 0.8) for fuel cell applications
by: Guo, Y., et al.
Published: (2009)
by: Guo, Y., et al.
Published: (2009)
Evaluation of (Ba 0.5Sr 0.5) 0.85Gd 0.15Co 0.8Fe 0.2O 3-[delta] cathode for intermediate temperature solid oxide fuel cell
by: Li, Z., et al.
Published: (2012)
by: Li, Z., et al.
Published: (2012)
Magnetotransport and electrical properties of colossal magnetoresistive La0.8Sr0.2Mn03 at different sintering temperature.
by: Lim, Kean Pah, et al.
Published: (2011)
by: Lim, Kean Pah, et al.
Published: (2011)
A Fundamental Study of Boron Deposition and Poisoning of La0.8Sr0.2MnO3 Cathode of Solid Oxide Fuel Cells under Accelerated Conditions
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Enhanced Chromium Tolerance of La0.6Sr0.4Co0.2Fe0.8O3-δ Cathode by BaO Infiltration
by: Chen, K., et al.
Published: (2015)
by: Chen, K., et al.
Published: (2015)
Composite cathode La0.4Sr0.4TiO3-[delta]- Ce0.8Sm0.2O2-[delta] impregnated with Ni for high-temperature steam electrolysis
by: Gan, Y., et al.
Published: (2014)
by: Gan, Y., et al.
Published: (2014)
Performance evaluation of an anode-supported solid oxide fuel cell with Ce0.8Sm0.2O1.9 impregnated GdBaCo2O5+d cathode
by: Wei, Bo, et al.
Published: (2012)
by: Wei, Bo, et al.
Published: (2012)
Sr2Fe1.5Mo0.5O6-δ - Sm0.2Ce0.8O1.9 Composite Anodes for Intermediate-Temperature Solid Oxide Fuel Cells
by: He, Beibei, et al.
Published: (2012)
by: He, Beibei, et al.
Published: (2012)
Further performance improvement of Ba0.5Sr0.5Co0.8Fe0.2O3-8 pervoskite membranes for air separation
by: Chen, Z., et al.
Published: (2009)
by: Chen, Z., et al.
Published: (2009)
Atenuasi ultrasonik dan modulus ricih pada suhu genting superkonduktor terdop sederhana (Tl0.8Bi0.2)Sr2 (Ca0.9Cr0.1)Cu2 O7
by: R. Abd-Shukor,, et al.
Published: (2022)
by: R. Abd-Shukor,, et al.
Published: (2022)
Similar Items
-
Performance and structural stability of Gd0.2Ce0.8O1.9 infiltrated La0.8Sr0.2MnO3 nanostructured oxygen electrodes of solid oxide electrolysis cells
by: Chen, Kongfa, et al.
Published: (2014) -
A comparative study of La0.8Sr0.2MnO3 and La0.8Sr0.2Sc0.1Mn0.9O3 as cathode materials of single-chamber SOFCs operating on a methane-air mixture
by: Zhang, C., et al.
Published: (2009) -
Ce0.9Gd0.1O2−δ membranes coated with porous Ba0.5Sr0.5Co0.8Fe0.2O3−δ for oxygen separation
by: Zhang, C., et al.
Published: (2015) -
Chromium deposition and poisoning in dry and humidified air at (La0.8Sr0.2)0.9MnO3+d cathodes of solid oxide fuel cells
by: Chen, X., et al.
Published: (2010) -
Properties and performance of Ba0.5Sr0.5Co0.8Fe0.2O3-d + Sm0.2Ce0.8O1.9 composite cathode
by: Wang, K., et al.
Published: (2008)