Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats

The characteristics of the X-ray attenuation in electrospun nano(n)- and micro(m)-Bi2O3/polylactic acid (PLA) nanofibre mats with different Bi2O3 loadings were compared as a function of energy using mammography (i.e. tube voltages of 22–49 kV) and X-ray absorption spectroscopy (XAS) (7–20 keV). Resu...

Full description

Bibliographic Details
Main Authors: Noor Azman, Nurul, Siddiqui, Salim, Haroosh, Hazim, Albetran, Hani, Johannessen, B., Dong, Yu, Low, It
Format: Journal Article
Published: Blackwell Publishing 2013
Subjects:
Online Access:http://hdl.handle.net/20.500.11937/20478
_version_ 1848750315730370560
author Noor Azman, Nurul
Siddiqui, Salim
Haroosh, Hazim
Albetran, Hani
Johannessen, B.
Dong, Yu
Low, It
author_facet Noor Azman, Nurul
Siddiqui, Salim
Haroosh, Hazim
Albetran, Hani
Johannessen, B.
Dong, Yu
Low, It
author_sort Noor Azman, Nurul
building Curtin Institutional Repository
collection Online Access
description The characteristics of the X-ray attenuation in electrospun nano(n)- and micro(m)-Bi2O3/polylactic acid (PLA) nanofibre mats with different Bi2O3 loadings were compared as a function of energy using mammography (i.e. tube voltages of 22–49 kV) and X-ray absorption spectroscopy (XAS) (7–20 keV). Results indicate that X-ray attenuation by electrospun n-Bi2O3/PLA nanofibre mats is distinctly higher than that of m-Bi2O3/PLA nanofibre mats at all energies investigated. In addition, with increasing filler loading (n-Bi2O3 or m-Bi2O3), the porosity of the nanofibre mats decreased, thus increasing the X-ray attenuation, except for the sample containing 38 wt% Bi2O3 (the highest loading in the present study). The latter showed higher porosity, with some beads formed, thus resulting in a sudden decrease in the X-ray attenuation.
first_indexed 2025-11-14T07:34:53Z
format Journal Article
id curtin-20.500.11937-20478
institution Curtin University Malaysia
institution_category Local University
last_indexed 2025-11-14T07:34:53Z
publishDate 2013
publisher Blackwell Publishing
recordtype eprints
repository_type Digital Repository
spelling curtin-20.500.11937-204782017-09-13T13:48:57Z Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats Noor Azman, Nurul Siddiqui, Salim Haroosh, Hazim Albetran, Hani Johannessen, B. Dong, Yu Low, It micro-Bi2O3/PLA thin films nano-Bi2O3/PLA thin films electrospun micro-Bi2O3/PLA nanofibre mat electrospun nano-Bi2O3/PLA nanofibre mat X-ray attenuation porosity The characteristics of the X-ray attenuation in electrospun nano(n)- and micro(m)-Bi2O3/polylactic acid (PLA) nanofibre mats with different Bi2O3 loadings were compared as a function of energy using mammography (i.e. tube voltages of 22–49 kV) and X-ray absorption spectroscopy (XAS) (7–20 keV). Results indicate that X-ray attenuation by electrospun n-Bi2O3/PLA nanofibre mats is distinctly higher than that of m-Bi2O3/PLA nanofibre mats at all energies investigated. In addition, with increasing filler loading (n-Bi2O3 or m-Bi2O3), the porosity of the nanofibre mats decreased, thus increasing the X-ray attenuation, except for the sample containing 38 wt% Bi2O3 (the highest loading in the present study). The latter showed higher porosity, with some beads formed, thus resulting in a sudden decrease in the X-ray attenuation. 2013 Journal Article http://hdl.handle.net/20.500.11937/20478 10.1107/S0909049513017871 Blackwell Publishing fulltext
spellingShingle micro-Bi2O3/PLA thin films
nano-Bi2O3/PLA thin films
electrospun micro-Bi2O3/PLA nanofibre mat
electrospun nano-Bi2O3/PLA nanofibre mat
X-ray attenuation
porosity
Noor Azman, Nurul
Siddiqui, Salim
Haroosh, Hazim
Albetran, Hani
Johannessen, B.
Dong, Yu
Low, It
Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats
title Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats
title_full Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats
title_fullStr Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats
title_full_unstemmed Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats
title_short Characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats
title_sort characteristics of x-ray attenuation in electrospun bismuth oxide/polylactic acid nanofibre mats
topic micro-Bi2O3/PLA thin films
nano-Bi2O3/PLA thin films
electrospun micro-Bi2O3/PLA nanofibre mat
electrospun nano-Bi2O3/PLA nanofibre mat
X-ray attenuation
porosity
url http://hdl.handle.net/20.500.11937/20478